Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 170 °C | 338 °F | Wet; DMA |
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 3K PW G30-500 Reinforced Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 0160 Unsaturated Polyester UP BMC 0160 is a general purpose BMC for electrical applications. Typical applications are lamp housings, canopies, covers and similar components.Information Provided by Menzolit |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 0170 Unsaturated Polyester UP BMC 0170 is a general purpose BMC for electrical applications. Product according to type 801 DIN 16911. The glass content is on a level that combines good mouldability with good strength and stiffne.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 0200 Unsaturated Polyester UP BMC 0200 is a standard BMC for general purpose applications. The glass content is on a level that combines good mouldability with good strength and stiffness properties. Even without a specific fire.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® MMC 1600 Unsaturated Polyester UP MMC 1600 is a mineral moulding compound (similar to DMC/BMC) providing of a stone like appearance eg. granite or marble. Chrome plated mould surfaces are required. It is recommended that product thi.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0170 Unsaturated Polyester UP SMC 0170 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0390 Unsaturated Polyester UP SMC 0390 is a standard low profile SMC. Because of its low shrinkage, the material shows good surface quality as well as very low warpage. The product is suitable for applications if a better surfac.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0600 Unsaturated Polyester UP SMC 0600 is a specially formulated SMC for reduced moulding pressure (< 30 bar). The glass level has been selected to combine good mouldability with strength and stiffness. Even without a specific f.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0650 Unsaturated Polyester UP SMC 0650 Low pressure SMC for large panels when moulding force becomes critical. Specific moulding pressure < 20 bar. A Special molding procedure is necessary.Information Provided by Menzolit |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 1650 Unsaturated Polyester UP SMC 1650 is a specially designed anti-microbial polyester moulding compound which incorporates a "germ killer" . It has been tested and found to be compliant for resistance to fungal defacement in .. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 2300 Unsaturated Polyester UP SMC 2300 is an arc resistance SMC for arc quenching cambers. High fire retardancy SMC for electrical applications .Information Provided by Menzolit |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 2600 Unsaturated Polyester UP SMC 2600 is a special SMC with electrically conductive properties. Because of its conductivity, SMC 2600 is antistatic and prevents build-up of electrical charges on the surface. Despite of its cond.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 0190 Unsaturated Polyester UP BMC 0190 is a general purpose BMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The flammability me.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 2800 Unsaturated Polyester UP BMC 2800 is a high performance BMC for matching the demands of medium and high voltage applications in the electrical field especially in respect of RTI 160+ according to Underwriters Laboratories .. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 2900 Unsaturated Polyester UP BMC 2900 is a specially designed BMC to meet the EC Safety Signs Directive (92/58/EEC) on the provision and use of safety signs at work. In areas where it is not possible to include the use of illu.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 2910 Unsaturated Polyester UP BMC 2910 incorporates additives which enhance the integral performance of mouldings during and after fire, currently used to mould Boltcaps which are designed to provide protection to the bolted co.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 3000 Unsaturated Polyester UP BMC 3000 is a special BMC suitable for the use in microwave and cookware applications.It has high temperature resistance, and meets requirements for food contact applications. It has a high gloss fi.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0150 Unsaturated Polyester UP SMC 0150 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0160 Unsaturated Polyester UP SMC 0160 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets .. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0190 Unsaturated Polyester UP SMC 0190 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0290 Unsaturated Polyester UP SMC 0290 is a specially formulated SMC processable by injection moulding. The gentle production process prevents the fiber from any damage. Parts made of SMC 0290 reach higher levels of strength and.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0300 Unsaturated Polyester UP SMC 0300 is a low shrink standard SMC providing improved surface quality, reduced shrinkage and warpage. Typical fields of applications are mechanical engineering and electrical industry, where impr.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 2500 Unsaturated Polyester UP SMC 2500 is a special SMC for high voltage isolating applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Even without a specific.. |
|||
Glass Transition Temp, Tg | >= 170 °C | >= 338 °F | |
Master Bond EP62-1Med USP Class VI Two Component Epoxy Resin System Master Bond EP62-1Med is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a 100 to 10 mi.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | DSC; IPC TM-650 2.4.25 |
Arlon 49N Multifunctional Epoxy Low-Flow Prepreg 49N is a low-flow epoxy prepreg engineered for bonding multilayer epoxy rigid-flex or attaching heat sinks to multilayer PCBs. With a high Tg, the prepreg can be used in high-performance or high-te.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | DSC; IPC TM-650 2.4.25 |
Arlon 45NK Woven Kevlar® Reinforced Laminate and Prepreg 45NK is a woven Kevlar® aramid fiber reinforced multifunctional epoxy laminate system engineered to provide in-plane CTE values as low as 6 ppm/°C for compatibility with leadless alumina ceramic c.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | DSC; IPC TM-650 2.4.25 |
Arlon 51N Lead-Free Compatible Epoxy Low-Flow 51N is a non-DICY multifunctional epoxy low-flow prepreg system designed to provide high reliability through lead-free solder operations. The high decomposition temperature and high thermal stabili.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | TMA; Nominal; IPC-TM-650.2.4.24c |
Park Electrochemical Nelco® N4000-6 FC Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-6 FC is a high-Tg epoxy laminate and prepreg system that provides a wide range of performance versatility and ease of processing for demanding high-layer count applications.Key Fea.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | DMA Method; IPC-TM-650 2.4.24 |
Rogers Corporation 2929 Bondply Unreinforced, Hydrocarbon based Thin Film Adhesive System Low dielectric constant and loss tangentIdeal for multi-layer bondingCompatible with traditional processing methodsCompatible with a broad range of material types including PTFE compositesReliable t.. |