Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 150 °C | 302 °F | ASTM D3482 |
Ovation Polymers Nemcon™ H PK DP110/X5 PEEK Thermally Conductive Polyetheretherketone, excellent chemical, high stiffness, modulus and HDT.Information provided by Ovation Polymers |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire PEEK is produced to the highest industry standards and .. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | ASTM D3417 |
Solvay Specialty Polymers KetaSpire® KT-850P Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-850P is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire PEEK is produced to the highest industry standa.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 450PF Fine Powder Grade Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, standard flow, FDA food contact complia.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | |
Cookson Group Plaskon® 3400FP Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A fast curing, reduced-stress epoxy molding compound for the encapsulation of semiconductor devices including DIPs, PLCCs, SOICs .. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | |
Cookson Group Plaskon® S-7P Epoxy Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, low viscosity epoxy encapsulant designed for packaging stress-sensitive semiconductor devices. It is specifically .. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 1800 Unsaturated Polyester UP SMC 1800 is for structural applications requiring extreme high mechanical properties and low weight. These compounds mould to parts focussing on mechanical strength for replacement of metals in ord.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | |
Ineos ABS Lustran® SMA 245 SMA Copolymer Lustran® SMA 245 is a Styrene Maleic Anhydride copolymer manufactured at a target maleic anhydride level of 25%. The process used for making Lustran® SMA 245 yields a product with good clarity.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | DSC |
Solvay Specialty Polymers Ajedium™ KT-820 Polyetheretherketone (PEEK) KetaSpire® KT-820 PEEK film is thermoplastic film that is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, high pu.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | DSC |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber KetaSpire® KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanic.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-820FP Polyetheretherketone (PEEK) KetaSpire® KT-820FP is the low-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color fine powder form suitable for compression molding. KetaSpire® PEEK is produced.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-820P Polyetheretherketone (PEEK) KetaSpire® KT-820P is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industry standards.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK) KetaSpire® KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire® PEEK is produced to the highest industry standa.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-850P Polyetheretherketone (PEEK) KetaSpire® KT-850P is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industr.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK) KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Ultimate Tg |
Tra-Con Tra-Bond F211 General Purpose Fiber Optic Epoxy Adhesive TRA-BOND F211 is a general purpose fiber optic epoxy adhesive recommended for bonding and small volume potting applications where superior wetting and physical properties are needed at both high and.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 381G Medium Viscosity Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F.. |