Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3418 |
NatureWorks® Ingeo™ 2003D General Purpose Transparent Extrusion Grade Biopolymer NatureWorks® PLA polymer 2003D is a thermoplastic resin derived from annually renewable resources. PLA polymer 2003D processes easily on conventional extrusion equipment. Specifically designed fo.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3418 |
NatureWorks® Ingeo™ 3052D Lubricated, High Flow Biopolymer NatureWorks® PLA polymer 2003D is a thermoplastic resin derived from annually renewable resources. It is designed for injection molding applications where the requirements are clarity with heat def.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6202D Fiber Grade PLA NatureWorks® PLA polymer 6202D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6202D is designed for extrusion into mechanically .. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6204D Fiber Grade PLA NatureWorks® PLA polymer 6204D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6204D is designed for extrusion into mechanically .. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6251D Fiber Grade PLA NatureWorks® PLA polymer 6251D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6251D is designed for spunbond products using conv.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6751D Fiber Grade PLA NatureWorks® PLA polymer 6751D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6751D is designed for extrusion into mechanically .. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 7032D Stretch Blow Molding/Bottle Grade PLA NatureWorks® PLA polymer 7032D is a bottles grade resin designed for injection stretch blow molded applications where heat setting is needed. PLA polymer 7032D can be run on conventional ISBM equip.. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | DSC, both heating and cooling speeds of 20°C/min |
Noltex Soarnol® AT4403 Ethylene Vinyl Alcohol Copolymer High ethylene content, low melting point. Suitable for use in multilayer structures where ease of thermoforming is required. Ethylene content 44 mol%.The gas barrier property of Soarnol is about fo.. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Crastin® S600F20 NC010 PBT
(Unverified Data**) Crastin® S600F20 NC010 is an unreinforced, lubricated, medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Crastin® S600F40 NC010 PBT
(Unverified Data**) Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6252D Meltblown Fiber Grade Biopolymer NatureWorks® PLA polymer 6252D is a thermoplastic fiber-grade resin derived from annually renewable resources. Available in lubricated pellet form, 6252D is designed for meltblown products using co.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6350D Fiber Grade PLA NatureWorks PLA polymer 6350D is an amorphous thermoplastic spunbond-grade resin derived primarily from annually renewable resources. Available in pellet form, 6350D is designed for extrusion into s.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6400D Fiber Grade PLA NatureWorks® PLA polymer 6400D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6400D is designed for extrusion into mechanically .. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | Dynamic Viscoelasticity |
EVALCA EVAL® LC-E105A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, melt phase forming, solid phase pressure forming, tubes, coex coating. EVOH is used in packaging applications because of its out.. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | ETM 300-90 |
ExxonMobil ESCOREZ™ 5300 Petroleum Hydrocarbon Resin The Escorez 5300 series resins are water white cycloaliphatic hydrocarbon resins. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, APP an d A.. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Crastin® FGS600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Food Contact Applications Crastin FGS600F40 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for injection .. |
|||
Glass Transition Temp, Tg | >= 55.0 °C | >= 131 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® 302-3M Optically Transparent Epoxy Product Description: EPO-TEK® 302-3M is a two component epoxy used for optical, medical, fiber optic, and semiconductor applications. The epoxy is good for adhesive joining, sealing, potting, or as.. |
|||
Glass Transition Temp, Tg | >= 55.0 °C | >= 131 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® 320 Optical, Opaque Epoxy Product Description: EPO-TEK® 320 is a two component, black-colored and optically opaque epoxy designed for optical, medical, and optoelectronic packaging of semiconductor devices and components. .. |
|||
Glass Transition Temp, Tg | >= 55.0 °C | >= 131 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® 320-LV Optically Opaque Epoxy Material Description: A two component, optically opaque epoxy adhesive designed for semiconductor and PCB applications in optoelectronic instrumentation and assemblies. A lower viscosity version of.. |
|||
Glass Transition Temp, Tg | >= 55.0 °C | >= 131 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® 730 General Purpose Epoxy Product Description: EPO-TEK® 730 is a two component, thixotropic, room temperature-curing epoxy adhesive. Advantages & Application Notes: Excellent all purpose adhesive. Many uses in job shop and .. |
|||
Glass Transition Temp, Tg | >= 55.0 °C | >= 131 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® OE121 Black Epoxy Adhesive Material Description: A two component, low temperature curing epoxy adhesive designed for semiconductor flip chip underfill. It is color coded black for visual ID during the underfilling process. .. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | |
Armstrong C-7/W Epoxy Adhesive, 1:1 Mix Ratio A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may .. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | |
3M Scotch-Weld™ 183 B/A Green Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir.. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | TM R050-25 |
Resinlab® EP1285HD-14 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Glass Transition Temp, Tg | 55.0 - 132 °C | 131 - 270 °F | Average value: 92.8 °C Grade Count:6 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | TM R050-25 |
Resinlab® EP1115 Clear Unfilled Epoxy Adhesive Resinlab™ EP1115 Clear is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and.. |