Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 225 °C | 437 °F | ASTM D3482 |
Ovation Polymers UTTAP™ SF 50030 GF Polyether Sulfone, 30% Glass Fiber Excellent chemical and electrical resistance, high stiffness, modulus and HDTAll properties after 48hrs conditioning at 23°C/50% RH |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ASTM D3482 |
Gharda Chemicals Gafone™ 3100 Polyethersulfone (PES)
(discontinued **) Characteristics: Excellent Thermal Resistance - Tg 224°C Outstanding Mechanical, Electrical, Flame & Chemical Resistance Very good Hydrolytic & Sterilization Resistance Good Optical Cl.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ASTM D3482 |
Gharda Chemicals Gafone™ 3610GM20 Polyethersulfone (PES)
(discontinued **) Characteristics: Excellent Thermal Resistance - Tg 224°C Outstanding Mechanical, Electrical, Flame & Chemical Resistance Very good Hydrolytic & Sterilization Resistance Good Optical Cl.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
Cookson Group Plaskon® SMT-B-1RC (146.403) Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for PBGA applications. It has the same unique resin system as SMT-B-1, which mi.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5001 PEI (Asia Pacific) Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5001 PEI (Europe-Africa-Middle East) Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones.Resin is RoHS compliant. UL94 V0 listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5011 PEI (Asia Pacific) Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5011R PEI (Asia Pacific) Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5111 PEI (Asia Pacific) 10% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5 VA listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5201 PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5201 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS compliant. UL94 V0 and 5VA li.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5201R PEI 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5201R PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics Ultem CRS5211 PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing.Thi.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5211R PEI 20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5211R PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5301 PEI 30% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5311 PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5311 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS compliant. UL94 V0 and 5VA li.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM CRS5711 PEI (Asia Pacific) 15% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
SABIC Innovative Plastics ULTEM UF5011S PEI (Europe-Africa-Middle East) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | |
Master Bond EP17HT-LO One component epoxy system for bonding, sealing, coating and casting Product Description: Master Bond EP17HT-LO is a one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation pr.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ISO 11357-1/-3 |
BASF Ultrason E 6020 P PES Ultrason E 6020 P is an unfilled, injection molding PES grade. Polyethersulfone flakes of high molecular weight and good solubility in typical solvents (N-Methylpyrrolidone, Dimethylacetamide, Dichl.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ISO 11357-1/-2 |
BASF Ultrason® E 2020 P SR PESU Description: Polyethersulfone flakes, e.g. for membrane applications, coatings and resin modification, containing min. 50% of OH-endgroups. The product is soluble in N-methyl-pyrrolidone (NMP) and N.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ISO 11357-1/-3 |
BASF Ultrason E 2010 PES Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ISO 11357-1/-2 |
BASF Ultrason® E 2010 HC PESU Information provided by BASF |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ISO 11357-1/-2 |
BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, .. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | ASTM D3482 |
Gharda Chemicals Gafone™ B2315GF Polysupersulfone (PSS)
(discontinued **) Characteristics: Excellent Dimensional properties Transparent Improved Impact Strength and Toughness as compared to PES Excellent Hydorlytic Stability High Stress Cracking Resistance Good Chemical.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | DSC |
Gharda Chemicals GAFONE™ 3430GF PES, Glass Fiber-Reinforced
(discontinued **) Glass fiber reinforced granules for injection molding. With lower viscosity for molding intricate cross sections.Characteristics: Very high rigidityGood dielectric propertiesHigh mechanical strengt.. |
|||
Glass Transition Temp, Tg | 225 °C | 437 °F | 10 K/min; ISO 11357-1/-2 |
BASF Ultrason E 2020 P PES Ultrason E 2020 P is an unfilled, injection molding PES grade. Polyethersulfone flakes, for solvent based processes; product is soluble e.g. in N-Methylpyrrolidone and N,N-Dimethylacetamide. |