Polymer Property : Specific Heat Capacity = 0.382 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
ASTM E1269
Eastman 9921P PET Film  (discontinued **)
Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia..
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
ASTM E1269
Eastman 9921P PET Injection Molded  (discontinued **)
Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia..
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer  (discontinued **)
Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i..
Specific Heat Capacity 1.60 - 1.60 J/g-°C

@Temperature 100 - 100 °C
0.382 - 0.382 BTU/lb-°F

@Temperature 212 - 212 °F
Average value: 1.60 J/g-°C Grade Count:21
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
ASTM C351
Solvay Specialty Polymers Ajediumâ„¢ PVDF 9009 Polyvinylidene Fluoride (PVDF)
Solef® 9009 PVDF homopolymer is a semi-crystalline fluoropolymer. Solef® film is chemically inert to most acids, aliphatic and aromatic organic compounds, chlorinated solvents and alcohols.Fea..
Specific Heat Capacity 1.60 J/g-°C
0.382 BTU/lb-°F
DSC
Eastman Eastobond 19411 Copolyester, Film
Eastobond 19411 is a terephthalate-based copolyester which is amorphous. It offers excellent organoleptic and gas-barrier properties. Eastobond 19411 has low postextrusion crystallinity and a low so..
Specific Heat Capacity 1.60 J/g-°C
0.382 BTU/lb-°F
DSC
Eastman Eastobond 19412 Copolyester, Film
Eastobond 19412 is a terephthalate-based copolyester. It is identical to our 19411 resin in every aspect, except that the 19412 has been crystallized for drying purposes and ease of handling. Eastob..
Specific Heat Capacity 1.60 J/g-°C
0.382 BTU/lb-°F
DSC
Eastman Neostar FN005 Elastomer
Neostar FN005 elastomer is a tough, clear, durable copolyester ether. It was designed for use in the profile and automotive markets, but is also used in packaging and tubing applications where tough..
Specific Heat Capacity 1.60 J/g-°C
0.382 BTU/lb-°F
DSC
Eastman Neostar FN007 Elastomer
Neostar FN007 elastomer is the third in Eastman’s series of tough, clear, durable copolyester ethers. Though originally designed for use in the profile and automotive markets, this innovative copol..
Specific Heat Capacity 1.60 J/g-°C
0.382 BTU/lb-°F
Melt
Covestro Makrolon® 8315 Polycarbonate, 10% Glass Filled
MVR (300 °C/1.2 kg) 6.0 cm3/10 minhigh viscosityeasy releaseinjection moldingavailable in opaque colors onlyPreprocessingMax. Water content
Specific Heat Capacity 1.60 J/g-°C
0.382 BTU/lb-°F
Melt
Covestro Makrolon® 9415 Polycarbonate, 10% Glass Filled
ISO 7391-PC,MFR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityEasy rel..
Specific Heat Capacity 1.60 J/g-°C
0.382 BTU/lb-°F
Melt
Covestro Makrolon® GF9002* Polycarbonate, 10% Glass Filled
ISO 7391-PC,MFR,(,,)-18-9,GF10Formerly Makrolon DP1-1889MVR (300 °C/1.2 kg) 15 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.2 mmUL 94 5VA/2.8 mm (Bayer ..
Specific Heat Capacity 1.60 J/g-°C
0.382 BTU/lb-°F
Melt
Covestro Makrolon® DP1-1887* Polycarbonate, 10% Glass Filled
ISO 7391-PC,MR,(,,)-18-9,GF10Developmental productMVR (300 °C/1.2 kg) 16 cm3/10 min10 % Glass fiber reinforcedMilled fiberLow viscosityEasy releasegood surface qualityInjection molding - Melt tempe..
Specific Heat Capacity 1.60 J/g-°C
0.382 BTU/lb-°F
IEC 1006
BASF Ultradur B 4040 G10 BK5110 50% Glass Filled PBT
Injection-molding grades containing 50% of glass fibers, for industrial parts with excellent surface quality.Applications: External door handles in vehicles, visible sunroof frames, over door handle..
Specific Heat Capacity 1.60 J/g-°C
0.382 BTU/lb-°F
IEC 1006
BASF Ultradur® B 4406 G2 10% Glass Filled PBT
Description: Is a PBT, flame-retardant injection-molding grades, with 10% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh..
Specific Heat Capacity 1.60 J/g-°C
0.382 BTU/lb-°F
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Dry)
Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat..
Specific Heat Capacity 1.60 J/g-°C
0.382 BTU/lb-°F
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Conditioned)
Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov..
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer  (discontinued **)
Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF ..
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
Solvay Specialty Polymers Solef® 1009 PVDF Homopolymer  (discontinued **)
Key features of this grade: Mean Viscosity, All Purpose, Injection/Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SO..
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
Solvay Specialty Polymers Solef® 11008 PVDF Copolymer  (discontinued **)
Key features of this grade: Low Viscosity, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVD..
Specific Heat Capacity 1.60 J/g-°C

@Temperature 100 °C
0.382 BTU/lb-°F

@Temperature 212 °F
Solvay Specialty Polymers Solef® 20810 PVDF Copolymer  (discontinued **)
Key features of this grade: Li Battery, Virgin. Recommended processing is solution. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta..
Copyright © lookpolymers.com All Rights Reserved