Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.80 J/g-°C @Temperature 200 °C |
0.430 BTU/lb-°F @Temperature 392 °F |
DSC |
Eastman Heatwave CF746 Polymer
(discontinued **) Heatwave is a clear, reheat enhanced, PET polyester designed for heatset containers containing a UV light protection package chemically bound to the backbone of the polymer. Pellets are 2.5 mm (0.1 .. |
|||
Specific Heat Capacity | 1.80 J/g-°C @Temperature 200 °C |
0.430 BTU/lb-°F @Temperature 392 °F |
ASTM E1269 |
Eastman Vitiva PC715 PET
(discontinued **) Vitiva PET PC715 is an exceptionally clear PET polyester that contains a UV light protection package chemically bound to the backbone of the polymer. This non-extractable UV inhibitor absorbs damagi.. |
|||
Specific Heat Capacity | 1.80 J/g-°C @Temperature 200 °C |
0.430 BTU/lb-°F @Temperature 392 °F |
ASTM E1269 |
Eastman Aqua 18696 PET
(discontinued **) Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Containers made from 186.. |
|||
Specific Heat Capacity | 1.80 J/g-°C @Temperature 200 °C |
0.430 BTU/lb-°F @Temperature 392 °F |
ASTM E1269 |
Eastman CM01 PET
(discontinued **) Voridian Polymer CM01 is clear polymer that is available in North America. This product is useful for production of beverage, food, and edible oil containers.Applications/UsesCarbonated soft drink c.. |
|||
Specific Heat Capacity | 1.80 J/g-°C @Temperature 200 °C |
0.430 BTU/lb-°F @Temperature 392 °F |
ASTM E1269 |
Eastman GP800 PET
(discontinued **) Voridian PET GP800 is a general purpose polymer that is available in the European, Middle East and Africa region. This product is developed for optimal production of PET bottles, containers, and fil.. |
|||
Specific Heat Capacity | 1.80 J/g-°C @Temperature 23.0 °C |
0.430 BTU/lb-°F @Temperature 73.4 °F |
DSC |
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont.. |
|||
Specific Heat Capacity | 1.80 J/g-°C | 0.430 BTU/lb-°F | |
Ineos Barex® 210 E Acrylonitrile-Methyl Acrylate Copolymer Extrusion Grade. Barex® Resins are available in either natural or blue tint. Barex® 210E is most commonly used for thermoformed sheet applications. |
|||
Specific Heat Capacity | 1.80 J/g-°C | 0.430 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Polidan® T/A-SP Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-SP is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Specific Heat Capacity | 1.80 J/g-°C @Temperature 125 °C |
0.430 BTU/lb-°F @Temperature 257 °F |
DSC |
Eastman Eastobond 19411 Copolyester, Film Eastobond 19411 is a terephthalate-based copolyester which is amorphous. It offers excellent organoleptic and gas-barrier properties. Eastobond 19411 has low postextrusion crystallinity and a low so.. |
|||
Specific Heat Capacity | 1.80 J/g-°C @Temperature 125 °C |
0.430 BTU/lb-°F @Temperature 257 °F |
DSC |
Eastman Eastobond 19412 Copolyester, Film Eastobond 19412 is a terephthalate-based copolyester. It is identical to our 19411 resin in every aspect, except that the 19412 has been crystallized for drying purposes and ease of handling. Eastob.. |
|||
Specific Heat Capacity | 1.80 J/g-°C @Temperature 100 °C |
0.430 BTU/lb-°F @Temperature 212 °F |
DSC |
Eastman Neostar FN005 Elastomer Neostar FN005 elastomer is a tough, clear, durable copolyester ether. It was designed for use in the profile and automotive markets, but is also used in packaging and tubing applications where tough.. |
|||
Specific Heat Capacity | 1.80 J/g-°C @Temperature 100 °C |
0.430 BTU/lb-°F @Temperature 212 °F |
DSC |
Eastman Neostar FN006 Elastomer Neostar FN006 elastomer is the second in Eastman’s series of tough, clear, durable copolyester ethers. Developed for use in the profile and automotive markets, it can also be used in packaging and .. |
|||
Specific Heat Capacity | 1.80 J/g-°C @Temperature 100 °C |
0.430 BTU/lb-°F @Temperature 212 °F |
DSC |
Eastman Neostar FN007 Elastomer Neostar FN007 elastomer is the third in Eastman’s series of tough, clear, durable copolyester ethers. Though originally designed for use in the profile and automotive markets, this innovative copol.. |
|||
Specific Heat Capacity | 1.80 J/g-°C | 0.430 BTU/lb-°F | Melt |
Covestro Bayblend® FR 3030 Polycarbonate + ABS, Flame Retardant Grade Flame retardant extrusion gradeVicat/B 120 temperature = 115 °Cgood extrusion and vacuum-forming behaviourUL-listing 94 V-0 (1.5 mm)halogen-free according to DIN VDE 0472-815glow wire temperature (.. |
|||
Specific Heat Capacity | 1.80 J/g-°C | 0.430 BTU/lb-°F | |
Dow ISONATE™ 125MDR Pure MDI ISONATE™ 125MDR is a crystalline, pure MDI mixture is characterized by high purity, low acidity and reproducible reactivity. This difunctional product is a key ingredient in preparing prepolymers .. |
|||
Specific Heat Capacity | 1.80 J/g-°C | 0.430 BTU/lb-°F | |
Dow ISONATE™ 143L Modified MDI ISONATE™ 143L modified MDI is a polycarbodiimide-modified diphenylmethane diisocyanate.Information provided by Dow |
|||
Specific Heat Capacity | 1.80 J/g-°C | 0.430 BTU/lb-°F | |
Dow ISONATE™ 143L Modified MDI ISONATE™ 143 is a polycarbodiimide-modified diphenylmethane diisocyanate. Liquid at room temperature, this product has a low viscosity and good storage stability down to 75°F. The polycarbodiimi.. |
|||
Specific Heat Capacity | 1.80 J/g-°C | 0.430 BTU/lb-°F | |
Dow ISONATE™ 181 MDI Prepolymer ISONATE™ 181 MDI prepolymer is a modified MDI compound produced by reacting high-purity diphenylmethane diisocyanate with sufficient glycol to allow easy handling down to 80°F. This medium-viscos.. |
|||
Specific Heat Capacity | 1.80 J/g-°C | 0.430 BTU/lb-°F | |
Dow ISONATE™ 240 MDI Prepolymer ISONATE™ 240 MDI prepolymer is a modified MDI compound produced by reacting high-purity diphenylmethane diisocyanate with a high molecular weight polyester polyol, resulting in a material with good.. |
|||
Specific Heat Capacity | 1.80 J/g-°C | 0.430 BTU/lb-°F | |
Dow ISONATE™ 50 O,P` Pure MDI ISONATE™ 50 O,P` is a high ortho-para MDI designed for use in polyurethane adhesives, sealants, sports flooring, coatings, electrical encapsulants and flexible molded foams. ISONATE™ 50 O,P` offe.. |
|||
Specific Heat Capacity | 1.80 J/g-°C | 0.430 BTU/lb-°F | |
Dow PAPI™ 901 Polymeric MDI PAPI™ 901 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product has a high functionality and a high viscosity resulting in highly rigid foams. This product is desi.. |
|||
Specific Heat Capacity | 1.80 J/g-°C | 0.430 BTU/lb-°F | |
Dow PAPI™ 94 Polymeric MDI PAPI™ 901 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This products low viscosity, low functionality, increased diphenylmethane diisocyanate content and increased perc.. |
|||
Specific Heat Capacity | 1.80 J/g-°C | 0.430 BTU/lb-°F | |
Dow ISONATE™ 181 MDI Prepolymer ISONATE™ 181 MDI prepolymer is a modified MDI compound produced by reacting high-purity diphenylmethane diisocyanate with sufficient glycol to allow easy handling down to 80°F. This medium-viscos.. |
|||
Specific Heat Capacity | 1.80 J/g-°C | 0.430 BTU/lb-°F | |
Dow PAPI™ 20 Polymeric MDI PAPI™ 20 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product`s functionality value of 3.2 and high viscosity result in highly rigid foams. This product is design.. |
|||
Specific Heat Capacity | 1.80 J/g-°C | 0.430 BTU/lb-°F | |
Dow PAPI™ 580 N Polymeric MDI PAPI™ 580 N polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product has high functionality (value of 3.0) and relatively high viscosity. Recommended for use in polyi.. |
|||
Specific Heat Capacity | 1.80 J/g-°C | 0.430 BTU/lb-°F | |
BASF Ultramid® A3WG3 15% Glass Filled PA66 (Dry) Description: 15% Glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of medium stiffness. For electric insulating parts, preference should be gi.. |
|||
Specific Heat Capacity | 1.80 J/g-°C | 0.430 BTU/lb-°F | |
Dow PAPI™ 27 Polymeric MDI PAPI™ 27 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product has a narrow molecular weight distribution and a high reactivity. Applicable to many foam processes,.. |
|||
Specific Heat Capacity | 1.80 J/g-°C @Temperature 200 °C |
0.430 BTU/lb-°F @Temperature 392 °F |
ASTM E1269 |
Eastman VersaTray 12822 Plastic
(discontinued **) VersaTray plastic 12822 is a polyethylene terephthalate resin designed for use as a base resin for crystallized PET (CPET) food trays and other high temperature food packaging applications. CPET foo.. |
|||
Specific Heat Capacity | 1.80 J/g-°C | 0.430 BTU/lb-°F | |
Styron Magnum™ 4435 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |
|||
Specific Heat Capacity | 1.80 - 2.03 J/g-°C | 0.430 - 0.485 BTU/lb-°F | Average value: 1.91 J/g-°C Grade Count:9 |
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and .. |