Eastman CM01 PET  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman CM01 PET  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Voridian Polymer CM01 is clear polymer that is available in North America. This product is useful for production of beverage, food, and edible oil containers.Applications/UsesCarbonated soft drink containersFood PackagingBottles
Physical Properties Metric English Comments
Bulk Density 0.858 g/cc
0.0310 lb/in³
Poured; ASTM D1895
0.931 g/cc
0.0336 lb/in³
Vibrated; ASTM D1895
Density 1.40 g/cc
0.0506 lb/in³
Crystalline Density; ASTM D1505
Melt Density 1.20 g/cc

@Temperature 285 °C
0.0434 lb/in³

@Temperature 545 °F
ASTM D1238
Viscosity Measurement 0.79 - 0.83
0.79 - 0.83
Intrinsic; EMN-A-AC-G-V-1
Thermal Properties Metric English Comments
Heat of Fusion 57.0 J/g
24.5 BTU/lb
ASTM E793
Specific Heat Capacity 1.10 J/g-°C
0.263 BTU/lb-°F
ASTM E1269
1.30 J/g-°C

@Temperature 80.0 °C
0.311 BTU/lb-°F

@Temperature 176 °F
ASTM E1269
1.50 J/g-°C

@Temperature 100 °C
0.359 BTU/lb-°F

@Temperature 212 °F
ASTM E1269
1.80 J/g-°C

@Temperature 200 °C
0.430 BTU/lb-°F

@Temperature 392 °F
ASTM E1269
2.00 J/g-°C

@Temperature 280 °C
0.478 BTU/lb-°F

@Temperature 536 °F
ASTM E1269
Melting Point 241 °C
466 °F
Crystalline Peak Melting Point; ASTM D3418
Descriptive Properties Value Comments
Acetaldehyde <1ppm
TEPO-A-AN-G-GC-67
Color, CIE a* -2.5 to 0.5
VGAS-A-AN-G-RS-001
Color, CIE b* -2.6 to -0.2
VGAS-A-AN-G-RS-001
Color, CIE L* 81 min
VGAS-A-AN-G-RS-001
Fines, wt%, max 0.1
VGAS-A-AN-G-GA-1
Pellet Shape Cylindrical, 2x2x3 mm