Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Parkway Products Thixomolded® AM50A Magnesium Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heate.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Zirconia Buster M-15 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.251 BTU/lb-°F | |
Zircar Zirconia Buster M2-35 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Zirconia Buster M-35 Alumina Board, Disc, and Cylinder Insulation Zircar alumina insulation Type Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with either a high purity alumina binder in BusterA-30 for use at 1600C or with s.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.251 BTU/lb-°F | |
Zircar Zirconia M-45 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | Average value: 1.05 J/g-°C Grade Count:8 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 100 °C |
0.250 BTU/lb-°F @Temperature 212 °F |
|
Kaiser 7068 T6, T651 Rod & Bar Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.251 BTU/lb-°F | |
Schwartz Technical Plastics LAMIGAMID® 510 Polyethylene Terephthalate Application: friction bearings, wear linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.251 BTU/lb-°F | DSC |
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics AL-30 Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics ALBF Alumina Bulk Fiber Alumina Bulk Fiber Type ALBF consists of long aluminum oxide fibers suited for the vacuum forming of low density shapes. The high alpha alumina content and addition of a grain growth inhibitor give .. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics ZAL-15AA Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Zirconia Buster A-30 Alumina Board, Disc, and Cylinder Insulation Zircar alumina insulation Type Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with either a high purity alumina binder in BusterA-30 for use at 1600C or with s.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Zirconia Buster M-15 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Zirconia Buster M-35 Alumina Board, Disc, and Cylinder Insulation Zircar alumina insulation Type Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with either a high purity alumina binder in BusterA-30 for use at 1600C or with s.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics Alumina Mat A layered, low density flexible mat made of 100% polycrystalline alumina fiber (non-RCF) designed for use to temperatures as high as 1650°C (3002°F). Shot free low density mat used as fill between.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.251 BTU/lb-°F | DuPont 990 test |
DuPont™ Tedlar® TWH20BS3 Satin White Polyvinyl Fluoride Film Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o.. |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 500 °C |
0.251 BTU/lb-°F @Temperature 932 °F |
|
3M Nextel™ AF-10 Aerospace Woven Fabric 312 Information provided by 3M |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 500 °C |
0.251 BTU/lb-°F @Temperature 932 °F |
|
3M Nextel™ AF-10 w/o sizing Aerospace Woven Fabric 312 Information provided by 3M |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 500 °C |
0.251 BTU/lb-°F @Temperature 932 °F |
|
3M Nextel™ AF-11 Industrial Woven Fabric 312 Information provided by 3M |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 500 °C |
0.251 BTU/lb-°F @Temperature 932 °F |
|
3M Nextel™ AF-11 w/o sizing Aerospace Woven Fabric 312 Information provided by 3M |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 500 °C |
0.251 BTU/lb-°F @Temperature 932 °F |
|
3M Nextel™ AF-20 Industrial Woven Fabric 312 Information provided by 3M |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 500 °C |
0.251 BTU/lb-°F @Temperature 932 °F |
|
3M Nextel™ AF-30 Industrial Woven Fabric 312 Information provided by 3M |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 500 °C |
0.251 BTU/lb-°F @Temperature 932 °F |
|
3M Nextel™ AF-40 Industrial Woven Fabric 312 Information provided by 3M |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 500 °C |
0.251 BTU/lb-°F @Temperature 932 °F |
|
3M Nextel™ AF-62 Industrial Woven Fabric 312 Information provided by 3M |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics AL-30AA Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics ALCAA Alumina Insulation ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form.Information provided by Zircar Ceramics. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics ZAL-15 Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics ZAL-45AA Alumina Insulation ZAL-45 is an exceptionally strong low density alumina fiber product. Alumina bonded ZAL-45AA is useful in reducing conditions.Information provided by Zircar Ceramics. |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 500 °C |
0.251 BTU/lb-°F @Temperature 932 °F |
|
3M Nextel™ AF-14 Industrial Woven Fabric 312 Information provided by 3M |