Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont™ Tedlar® TWH20BS3 Satin White Polyvinyl Fluoride Film

Category Polymer , Film , Thermoplastic , Fluoropolymer
Manufacturer DuPont
Trade Name Tedlar®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Tedlar® TWH20BS3 Satin White Polyvinyl Fluoride Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety of chemicals, solvents, and staining agents.Information provided by DuPont.
Physical Properties Metric English Comments
Specific Gravity 1.71 g/cc
1.71 g/cc
ASTM D1505
Moisture Absorption at Equilibrium <= 0.50 %
<= 0.50 %
ASTM D570
Moisture Vapor Transmission 0.860 cc-mm/m²-24hr-atm
2.18 cc-mil/100 in²-24hr-atm
ASTM E96
Thickness 50.8 microns
2.00 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD >= 110 %
>= 110 %
ASTM D882
Secant Modulus, MD 2.65 GPa
385 ksi
ASTM D822
Impact 71.6
71.6
kJ/m; Spencer; ASTM D3420
Coefficient of Friction 0.18
0.18
Film:Metal; ASTM D1894
Tear Strength 146 kN/m
833 pli
Graves (initial), TD; ASTM D1004
195 kN/m
1110 pli
Graves (initial), MD; ASTM D1004
Elmendorf Tear Strength, MD 1.82 g/micron
46.2 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 1.05 g/micron
26.6 g/mil
ASTM D1922
Film Tensile Strength at Break, MD >= 62.1 MPa
>= 9000 psi
ASTM D882
Thermal Properties Metric English Comments
CTE, linear 83.0 µm/m-°C

@Temperature 50.0 - 70.0 °C
46.1 µin/in-°F

@Temperature 122 - 158 °F
TD; ASTM D696
97.0 µm/m-°C

@Temperature 50.0 - 70.0 °C
53.9 µin/in-°F

@Temperature 122 - 158 °F
MD; ASTM D696
Specific Heat Capacity 1.05 J/g-°C
0.251 BTU/lb-°F
DuPont 990 test
Maximum Service Temperature, Air 107 °C
225 °F
Continuous
175 °C
347 °F
Short Cycle
Minimum Service Temperature, Air -72.0 °C
-97.6 °F
Continuous
Shrinkage <= 5.0 %

@Temperature 170 °C
<= 5.0 %

@Temperature 338 °F
TD; ASTM D1204
Optical Properties Metric English Comments
Refractive Index 1.46

@Temperature 30.0 °C
1.46

@Temperature 86.0 °F
n<sub>D</sub>; Abbe Refractometer; ASTM D-542
Electrical Properties Metric English Comments
Volume Resistivity 1.50e+11 ohm-cm

@Temperature 100 °C
1.50e+11 ohm-cm

@Temperature 212 °F
ASTM D257
7.00e+14 ohm-cm

@Temperature 22.0 °C
7.00e+14 ohm-cm

@Temperature 71.6 °F
ASTM D257
Dielectric Constant 11

@Frequency 1000 Hz
11

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 138 kV/mm

@Frequency 60.0 Hz
3500 kV/in

@Frequency 60.0 Hz
ASTM D150
Dissipation Factor 0.014

@Frequency 1000 Hz,
Temperature 22.0 °C
0.014

@Frequency 1000 Hz,
Temperature 71.6 °F
ASTM D150
0.016

@Frequency 10000 Hz,
Temperature 70.0 °C
0.016

@Frequency 10000 Hz,
Temperature 158 °F
ASTM D150
0.017

@Frequency 1000 Hz,
Temperature 70.0 °C
0.017

@Frequency 1000 Hz,
Temperature 158 °F
ASTM D150
0.034

@Frequency 10000 Hz,
Temperature 22.0 °C
0.034

@Frequency 10000 Hz,
Temperature 71.6 °F
ASTM D150
Descriptive Properties Value Comments
Aging in Air > 3000 hours to embrittlement
300°F Oven