Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.962 - 1.05 J/g-°C | 0.230 - 0.251 BTU/lb-°F | |
Polikim EFALON® T-100 Virgin PTFE Applications: Gaskets, seals, O-rings, V-Rings, compression packings and similar sealing parts, Bushes, bearings and piston rings, Electrical insulators, Sliding supports, Conveyor belts, Coated tu.. |
|||
Specific Heat Capacity | 0.962 J/g-°C | 0.230 BTU/lb-°F | |
Owens Corning Glass Fiber Reinforced Epoxy (Filament Wound), 80 wt.% glass Epoxies are highly resistant to water, alkalis and organic solvents. Although standard epoxies have only a fair resistance to acids and oxidizing agents, they can be formulated for better resistance.. |
|||
Specific Heat Capacity | 0.962 J/g-°C | 0.230 BTU/lb-°F | ASTM C351 |
Park Electrochemical Nelcote® F-554 Phenolic Prepreg, Chopped Molding Compound Reinforced Nelcote® F-554 is a high purity silica filled phenolic resin coated on Commercial or Aerospace grade silica fabric. F-554 is used in the manufacture of intermediate temperature ablative rocket nozz.. |
|||
Specific Heat Capacity | 0.962 J/g-°C | 0.230 BTU/lb-°F | ASTM E1461-92 |
Park Electrochemical Nelco® N4000-7 EF® Halogen-Free Epoxy The Nelco® N4000-7 EF® series of laminates and prepregs is a total environmental solution. This advanced halogen-free resin system provides superior CAF resistance for high temperature, lead-free .. |
|||
Specific Heat Capacity | 0.962 J/g-°C @Temperature 23.0 °C |
0.230 BTU/lb-°F @Temperature 73.4 °F |
ASTM D3418 |
Solvay Specialty Polymers Halar® 1400LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**) Information provided by Solvay Specialty Polymers. |
|||
Specific Heat Capacity | 0.962 J/g-°C @Temperature 23.0 °C |
0.230 BTU/lb-°F @Temperature 73.4 °F |
ASTM D3418 |
Solvay Specialty Polymers Halar® 1450LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**) Information provided by Solvay Specialty Polymers. |
|||
Specific Heat Capacity | 0.962 J/g-°C @Temperature 23.0 °C |
0.230 BTU/lb-°F @Temperature 73.4 °F |
ASTM D3418 |
Solvay Specialty Polymers Halar® 300DA Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Halar® "DA" grades are available and meet the FDA's Condition of Use B, as described under 21 C.F.R. 176-170(c).Information provided by Solvay Specialty Polymers. |
|||
Specific Heat Capacity | 0.962 J/g-°C @Temperature 23.0 °C |
0.230 BTU/lb-°F @Temperature 73.4 °F |
ASTM D3418 |
Solvay Specialty Polymers Halar® 300LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(discontinued **) Information provided by Solvay Specialty Polymers. |
|||
Specific Heat Capacity | 0.962 J/g-°C @Temperature 23.0 °C |
0.230 BTU/lb-°F @Temperature 73.4 °F |
ASTM D3418 |
Solvay Specialty Polymers Halar® 350LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Specific Heat Capacity | 0.962 J/g-°C @Temperature 23.0 °C |
0.230 BTU/lb-°F @Temperature 73.4 °F |
ASTM D3418 |
Solvay Specialty Polymers Halar® 5001C Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Powder grades for masterbatches.Information provided by Solvay Specialty Polymers. |
|||
Specific Heat Capacity | 0.962 J/g-°C @Temperature 23.0 °C |
0.230 BTU/lb-°F @Temperature 73.4 °F |
ASTM D3418 |
Solvay Specialty Polymers Halar® 500LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Specific Heat Capacity | 0.962 J/g-°C @Temperature 23.0 °C |
0.230 BTU/lb-°F @Temperature 73.4 °F |
ASTM D3418 |
Solvay Specialty Polymers Halar® 513LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
Specific Heat Capacity | 0.962 J/g-°C @Temperature 23.0 °C |
0.230 BTU/lb-°F @Temperature 73.4 °F |
ASTM D3418 |
Solvay Specialty Polymers Halar® 901 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)< Information provided by Solvay Specialty Polymers. |
|||
Specific Heat Capacity | 0.962 J/g-°C @Temperature 23.0 °C |
0.230 BTU/lb-°F @Temperature 73.4 °F |
ASTM D3418 |
Solvay Specialty Polymers Halar® 902 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)< Information provided by Solvay Specialty Polymers. |
|||
Specific Heat Capacity | 0.962 J/g-°C | 0.230 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Ajedium™ Films -- Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Halar® ECTFE is a semi-crystalline fluoropolymer with a chemical structure of a 1:1 alternating copolymer of ethylene and chlorotrifluoroethylene.Halar® film is a strong, hard, tough, abrasion.. |
|||
Specific Heat Capacity | 0.962 J/g-°C | 0.230 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Halar® 1400LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: FibersAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 300 °CInformation provided by Solvay Spec.. |
|||
Specific Heat Capacity | 0.962 J/g-°C | 0.230 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Halar® 1450LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polyme.. |
|||
Specific Heat Capacity | 0.962 J/g-°C | 0.230 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Halar® 300DA Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Halar® "DA" grades are available and meet the FDA's Condition of Use B, as described under 21 C.F.R. 176-170(c).Features: Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 .. |
|||
Specific Heat Capacity | 0.962 J/g-°C | 0.230 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Halar® 350LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Specific Heat Capacity | 0.962 J/g-°C | 0.230 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Halar® 5001C Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Powder grades for masterbatches.Features: Low ViscosityUses: Masterbatch; Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0.. |
|||
Specific Heat Capacity | 0.962 J/g-°C | 0.230 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation prov.. |
|||
Specific Heat Capacity | 0.962 J/g-°C | 0.230 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Halar® 513LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: MonofilamentsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solv.. |
|||
Specific Heat Capacity | 0.962 J/g-°C | 0.230 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Halar® 930LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Specific Heat Capacity | 0.962 J/g-°C | 0.230 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Halar® 930LCW Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Specific Heat Capacity | 0.962 J/g-°C | 0.230 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Halar® 901 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym.. |
|||
Specific Heat Capacity | 0.962 J/g-°C | 0.230 BTU/lb-°F | ASTM C351 |
Solvay Specialty Polymers Halar® 902 Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) High ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 28.0 J/g; Heat of Fusion - ASTM D3418 28.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polym.. |
|||
Specific Heat Capacity | 0.962 J/g-°C | 0.230 BTU/lb-°F | DSC |
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled
(discontinued **) AURUM JGN3030 is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, glass fiber .. |