Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | >= 340 °C | >= 644 °F | ISO 3146 |
Panjin Zhongrun Chemerize 085P Low Viscosity CoPEEK Information provided by Bieglo Gmbh. |
|||
Melting Point | >= 340 °C | >= 644 °F | ISO 3146 |
Panjin Zhongrun Chemerize 012P High Viscosity CoPEEK Information provided by Bieglo Gmbh. |
|||
Melting Point | 340 °C | 644 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Ketron® 1000 IM Injection Molded Unfilled Polyetheretherketone (ASTM Product Data Sheet) Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to hot water or steam |
|||
Melting Point | 340 °C | 644 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Ketron® 1000 PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Melting Point | 340 °C | 644 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Ketron® GF30 PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Melting Point | 340 °C | 644 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP Ketron® HPV PEEK + carbon fibres + PTFE + graphite, bearing grade, extruded (ISO Data) The addition of carbon fibres, PTFE and graphite to virgin PEEK results in a Ketron PEEK “bearing grade”. Its excellent tribological properties (low friction, long wear and high pressure-velocity .. |
|||
Melting Point | 340 °C | 644 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Semitron® MDS 100 (ASTM Product Data Sheet) |
|||
Melting Point | 340 - 372 °C | 644 - 702 °F | Average value: 347 °C Grade Count:6 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Melting Point | 340 °C | 644 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gra.. |
|||
Melting Point | >= 340 °C | >= 644 °F | ISO 3146 |
Panjin Zhongrun Chemerize 012G High Viscosity CoPEEK Information provided by Bieglo Gmbh. |
|||
Melting Point | 340 °C | 644 °F | ISO 11357 |
Quadrant EPP Ketron® LSG PEEK-CLASSIX Biocompatibility tested (ASTM Product Data Sheet) KETRON® PEEK-CLASSIX LSG white stock shapes are produced from Invibio® PEEK-CLASSIX White resin. This material exhibits a unique combination of mechanical properties, temperature and chemical re.. |
|||
Melting Point | >= 340 °C | >= 644 °F | |
Hong Kun Group DBDPE Flame Retardant Chemical Name:1,2-Bis(pentabromophenyl) ethaneDecabromodiphenylethaneDecabromodiphenyl EthylCAS No. 84852-53-9All information provided by Hongkun Group |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Solvay Specialty Polymers Ajedium™ Films -- AvaSpire® AV-630 Polyaryletherketone (PAEK) AvaSpire® AV-630 PAEK film is a unique thermoplastic film that is characterized by a distinct combination of properties, which include strength, ductility, fatigue resistance, high purity and exc.. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining.. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable.. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber KetaSpire® KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanic.. |
|||
Melting Point | 340 °C | 644 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-820P Polyetheretherketone (PEEK) KetaSpire® KT-820P is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industry standards.. |
|||
Melting Point | 340 °C | 644 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK) KetaSpire® KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire® PEEK is produced to the highest industry standa.. |
|||
Melting Point | 340 °C | 644 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK) KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and.. |
|||
Melting Point | 340 °C | 644 °F | DSC, Second Heating; ISO 11357 |
Westlake Plastics MediPEEK T Polyetheretherketone for Medical Applications MediPEEK-T is a high performance semi-crystalline thermoplastic designed for short term body contact as an implantable material. It is USP Class VI and ASTM F2026 compliant. It has excellent steri.. |
|||
Melting Point | 340 °C | 644 °F | ASTM D4591 |
Westlake Plastics PEEK PEEK is a high performance semi-crystalline thermoplastic. PEEK characteristics include high temperature performance, excellent wear properties, superior chemical resistance and outstanding toughne.. |
|||
Melting Point | 340 °C | 644 °F | DSC |
Westlake Plastics PEEK Film Made from VICTREX® Polymer Extremely high temperature resistance and continuous use temperature. Excellent flexural and tensile properties. Good abrasion and rain erosion resistance. Excellent chemical resistance. Excelle.. |
|||
Melting Point | 340 °C | 644 °F | DSC |
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut.. |
|||
Melting Point | 340 °C | 644 °F | |
Ensinger Tecapeek® MT Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |
|||
Melting Point | 340 °C | 644 °F | 10K/min; ISO 3146 |
CENTROPLAST CENTROPEEK Polyetheretherketone This plastic has high temperature resistance, good chemical resistance, and good mechanical characteristics. Its has good sliding friction properties and is suitable for use with foodstuffs or medi.. |
|||
Melting Point | 340 °C | 644 °F | DSC |
Gharda Chemicals GATONE™ 5300PF Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
Melting Point | 340 °C | 644 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. The .. |
|||
Melting Point | 340 °C | 644 °F | Peak; ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical strength a.. |
|||
Melting Point | >= 340 °C | >= 644 °F | ISO 3146 |
Panjin Zhongrun Chemerize 021G Medium Viscosity CoPEEK Information provided by Bieglo Gmbh. |
|||
Melting Point | 340 °C | 644 °F | Crystalline, Peak; ASTM D3418 |
Quadrant EPP Ketron® CM CA30 PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to ho.. |