Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 442 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 228 °C
442 °F
Indium Corp. Sn995 Cobalt-Doped, Pb-Free Soldering Alloy
Sn995 Cobalt-Doped Pb-Free Soldering Alloy is a cobalt-doped Sn/Cu alloy that provides a low cost alternative to traditional SAC305. In addition to the lower cost, this cobalt- and bismuth-doped Sn..
Melting Point 228 - 244 °C
442 - 471 °F
Limits; M2E-73-002
Indorama Ventures Mexico Polyclearâ„¢ T-94 PET Resin
Description: La resina Polyclear® PET T-94 de Arteva Specialities es un copolimero de baja velocidad de cristalizacion, ideal para la fabricacion de pared gruesa, con una viscosidad intrinseca de..
Melting Point 228 °C
442 °F
10°C/min; ISO 11357-1, -3
Lanxess Pocan® BF 4130 XF 000000 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding, flame retardant, improved flowabilityInformation provided by LANXESS.
Melting Point 228 °C
442 °F
10°C/min; ISO 11357-1/-3
Lanxess Pocan® BF 4130 XF 700051 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding, flame retardant, improved flowability
Melting Point <= 228 °C
<= 442 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 150AC Low Density Polyethylene Resin
Product Description: LD 150 series are LDPE grades, offering good blend mechanical properties and stiffness. Several additive packages are available according to the required surface properties.Avai..
Melting Point <= 228 °C
<= 442 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 150BW Low Density Polyethylene Resin
Product Description: LD 150 series are LDPE grades, offering good blend mechanical properties and stiffness. Several additive packages are available according to the required surface properties.Avai..
Melting Point <= 228 °C
<= 442 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 150BW Wire & Cable Low Density Polyethylene Resin
Product Description: LD 150BW is a LDPE containing suitable for the production of LV and MV crosslinked insulation using the 1-step or 2-step silane technology. Through in-house compounding it can a..
Melting Point <= 228 °C
<= 442 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 159AC Low Density Polyethylene Resin
Product Description: LD 159AC is an LDPE grade, which offers good draw down combined with good mechanical strength. Availability: Africa & Middle East and Europe Additive: Antiblock: 450 ppmSlip: 5..
Melting Point <= 228 °C
<= 442 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin (European Grade)
Product Description: LD 165 series are LDPE grades, offering high strength combined with medium optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoTherm..
Melting Point <= 228 °C
<= 442 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 201.48 Low Density Polyethylene Resin
Product Description: LD 201.48 is an LDPE extrusion coating grade, designed to have excellent processability combined with heat sealability and adhesion. It offers – Excellent neck-in/draw down bal..
Melting Point <= 228 °C
<= 442 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 252 Low Density Polyethylene Resin (European Grade)
Product Description: LD 525 is a high purity LDPE extrusion coating grade, designed to meet environmental needs for reduced fume emissions during plastics conversion. This grade offers:Low volatiles..
Melting Point <= 228 °C
<= 442 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 419.MV Low Density Polyethylene Resin
Product Description: LD 419.MV is a LDPE designed for wire and cable applications and is suitable for making crosslinkable compounds for medium voltage insulation.Availability: Latin America, North ..
Melting Point <= 228 °C
<= 442 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 600BA Low Density Polyethylene Resin (European Grade)
Product Description: LD 600BA is a high flow LDPE grade, characterized by high stiffness and good toughness. It’s easy processable.Availability: Africa & Middle East and Europe Additive: Antiblock..
Melting Point <= 228 °C
<= 442 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 653 Low Density Polyethylene Resin (European Grade)
Product Description: LD 653 is an easy flowing LDPE grade with medium stiffness and good toughness.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: ..
Melting Point 228 °C
442 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Sorona® 3301 BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&l
Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301 BK001 is an unreinforced black polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight w..
Melting Point 228 °C
442 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Sorona® 3301 NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&l
Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with su..
Melting Point 228 °C
442 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Sorona® 3301V BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301V BK001 is an unreinforced black polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight ..
Melting Point 228 °C
442 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Sorona® FG3301 NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)
Unreinforced Renewably Sourced Polytrimethylene Terephthalate Developed for Food Contact Applications Sorona FG3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renew..
Melting Point 228 °C
442 °F
STN EN 11357-1
Plastcom SLOVASTER® B GB 40 PBT reinforced with glass beads
PBT for injection molding, reinforced with 40% glass beads. Characterized by very good properties also at low temperature. Melt is characterized by very good rheology, which enables manufacturing of..
Melting Point 228 °C
442 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Sorona® 3301V NC010 Polytrimethylene Terephthalate (PTT)
Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301V NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight develo..
Melting Point 228 °C
442 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Sorona® 3301 BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&l
Sorona® 3301 BK001 is an unreinforced black polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with superior surface appearance in ambient temperature condi..
Melting Point 228 °C
442 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Sorona® 3301 NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&l
Sorona® 3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with superior surface appearance in ambient temperature conditions...
Melting Point 228 °C
442 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Sorona® 3301V BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
Sorona® 3301V BK001 is an unreinforced black polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight developed for applications requiring high surface gloss in a..
Melting Point 228 °C
442 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Sorona® 3301V NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
Sorona® 3301V NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight developed for applications requiring high surface gloss in a broad..
Melting Point 228 °C
442 °F
ASTM D3417
Quantum PEI - Ultem® 30% Glass Fiber Filled
Information provided by Quantum Advanced Engineering Plastics