Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer Indorama Ventures Mexico
Trade Name Polyclear™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indorama Ventures Mexico Polyclearâ„¢ T-94 PET Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: La resina Polyclear® PET T-94 de Arteva Specialities es un copolimero de baja velocidad de cristalizacion, ideal para la fabricacion de pared gruesa, con una viscosidad intrinseca de 0.86 dl/g. La resina Polyclear® PET T-94 tiene excelentes propiedades de cristalizacion y fundido, que facilita el proceso de inyeccion-estirado-soplado. La resina cumple con la regulación de la Federal Food, Drug and Cosmetic Act para aplicaciones especificas en alimentos. Para mayores detalles de la FDA, por favor contacte a Arteva Specialties. Los envases hechos con la resina Polyclear® PET T-94 son ligeros, irrompibles, tienen excelente brillo, transparencia y propiedades de barrera. Son atoxicos, se pueden pigmentar en una amplia gama de colores, y tienen la gran ventaja de ser totalmente reciclables.
Physical Properties Metric English Comments
Density >= 1.394 g/cc
>= 0.05036 lb/in³
Limit; M2E-71-043
1.398 g/cc
0.05051 lb/in³
Target; M2E-71-043
Apparent Bulk Density 0.900 g/cc
0.0325 lb/in³
Target; M2E-72-015
0.850 - 0.950 g/cc
0.0307 - 0.0343 lb/in³
Limit; M2E-72-015
Viscosity Measurement 0.86
0.86
Target; M2E-75-011
0.84 - 0.88
0.84 - 0.88
Limits; M2E-75-011
Crystallinity >= 45 %
>= 45 %
Limit; M2E-71-043
51 %
51 %
Target; M2E-71-043
Thermal Properties Metric English Comments
Melting Point 236 °C
457 °F
Target; M2E-73-002
228 - 244 °C
442 - 471 °F
Limits; M2E-73-002
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Chemical Properties Metric English Comments
Acetaldehyde 0.500 ppm
0.500 ppm
Target; M2E-75-007
<= 1.50 ppm
<= 1.50 ppm
Limit; M2E-75-007
Processing Properties Metric English Comments
Moisture Content 0.15 %
0.15 %
Target; M2E-72-010
<= 0.30 %
<= 0.30 %
Limit; M2E-72-010
Descriptive Properties Value Comments
Chip Size 65 to 95 No/g
Limits, M2E-75-004
80 No/g
Target, M2E-75-004
Color, CIE -5 (b)
Target, M2E-75-002
-6.5 to -3.5 (b)
Limits, M2E-75-002
Fines < 0.1%
M2E-76-033
Process Blow Molding
Injection Molding
Region Mexico
Bamberger Polymers Distribution
Yellow Chips < 9 No/125g
M2E-75-014