ExxonMobil LDPE LD 600BA Low Density Polyethylene Resin (European Grade)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Exxon Chemical
Trade Name LDPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LDPE LD 600BA Low Density Polyethylene Resin (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: LD 600BA is a high flow LDPE grade, characterized by high stiffness and good toughness. It’s easy processable.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: CapsClosuresCompoundingFood Packaging ContainersHouseware ArticlesInjection MoldingMasterbatch Base ResinTechnical PartsToysViscosity ModifierInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ExxonMobil method
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 190 °C
21 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 44
44
ISO 868
Tensile Strength at Break 8.96 MPa
1300 psi
ISO 527-2/1A/50
Elongation at Break 140 %
140 %
ISO 527-2/1A/50
Tensile Modulus 0.193 GPa
28.0 ksi
ISO 527-2/1A/1
Thermal Properties Metric English Comments
Melting Point <= 228 °C
<= 442 °F
Peak Melting Point; ExxonMobil method
Vicat Softening Point 91.1 °C
196 °F
ISO 306