Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 223 - 225 °C | 433 - 437 °F | |
Plastcom SLOVASTER® B/A GF 20 PBT, 20% glass fibre FeaturesPBT/ASA for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben.. |
|||
Melting Point | 223 °C | 433 °F | ISO 3146 |
PolyOne Bergamid™ B650 G/Mi20 UF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Melting Point | 223 °C | 433 °F | ISO 3146 |
PolyOne Bergamid™ B70 UF V2 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Melting Point | 223 °C | 433 °F | ISO 3146 |
PolyOne Bergamid™ B700 G20 H UF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Melting Point | 223 °C | 433 °F | ISO 3146 |
PolyOne Bergamid™ B700 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Melting Point | 223 - 227 °C | 433 - 441 °F | DSC |
Gromax CCP PBT 1100-211X Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melting Point | 223 °C | 433 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Crastin® CE15315 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin CE15315 NC010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0.. |
|||
Melting Point | 223 °C | 433 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Crastin® S610SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin S610SF is an unreinforced low viscosity polybutylene terephthalate for injection molding. It has hig.. |
|||
Melting Point | 223 °C | 433 °F | 10 K/min; ISO 3146 |
Eurotec® Tecomid® NB40 GR20 NL XA 20 PA 6 20% glass fiber reinforced, UL94 V0 Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Melting Point | 223 °C | 433 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NB40 GR30 NL MB PA6, 30% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 223 °C | 433 °F | 10 K/min; ISO 3146 |
Eurotec® Tecomid® NB40 GR40 NL PA 6 40% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Melting Point | 223 °C | 433 °F | 10 K/min; ISO 3146 |
Eurotec® Tecomid® NB40 GR50 NL PA 6 50% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Melting Point | 223 °C | 433 °F | 10 K/min; ISO 3146 |
Eurotec® Tecomid® NB40 NL XA 20 PA 6 unreinforced, UL94 V0 Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Melting Point | 223 °C | 433 °F | ISO 11357-1/-3 |
Covestro Makroblend® KU 2-7912 Polycarbonate + PBT, Impact Grade ISO 7792-1-PC/PBT,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding grademedium flowhigh toughness at low temperaturesideal for painted applicationunreinforcedPreprocessingMax. Water content |
|||
Melting Point | 223 °C | 433 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® MB40 GR20 NL PA6, 20% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Melting Point | 223 °C | 433 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NB40 GR15 NL HS PA6, 15% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 223 °C | 433 °F | 10 K/min |
BASF Ultradur B 2300 G6 HR BK15116 30% Glass Filled PBT Ultradur B 2300 G6 HR BK15116 is a hydrolysis resistant, pigmented black 30% fiberglass reinforced PBT, exhibiting superior flow characteristics. Designed for improved latch
strength in automotive.. |
|||
Melting Point | 223 °C | 433 °F | 10 K/min |
BASF Ultradur B 4300 G2 LS High Speed BK15045 10% Glass Filled PBT |
|||
Melting Point | 223 °C | 433 °F | 10 K/min |
BASF Ultradur B 4300 G4 BK5110 20% Glass Filled PBT Ultradur B 4300 G4 BK5110 is an easy flowing, pigmented black, injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts. |
|||
Melting Point | 223 °C | 433 °F | ASTM Test |
BASF Ultradur B 4300 G4 BK5110 20% Glass Filled PBT Ultradur B 4300 G4 BK5110 is an easy flowing, pigmented black, injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts. |
|||
Melting Point | 223 °C | 433 °F | 10 K/min |
BASF Ultradur B 4300 G4 LS High Speed BK15045 20% Glass Filled PBT |
|||
Melting Point | 223 °C | 433 °F | 10 K/min |
BASF Ultradur B 4406 G4 Q113 20% Glass Filled PBT Ultradur B4406 G4 Q113 is an UL V0 injection molding PBT grade with 20% glass fiber reinforcement. |
|||
Melting Point | 223 °C | 433 °F | ASTM Test |
BASF Ultradur B 4406 G6 BKQ113 7110 30% Glass Filled PBT Ultradur B 4406 G6 BKQ113 7110 is an UL V0 injection molding, pigmented black, PBT grade with 30% glass fiber reinforcement. |
|||
Melting Point | 223 °C | 433 °F | 10 K/min |
BASF Ultradur B 4406 G6 Q113 30% Glass Filled PBT Ultradur B4406 G6 Q113 is an UL V0 injection molding, PBT grade with 30% glass fiber reinforcement. |
|||
Melting Point | 223 °C | 433 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NB40 KG30NL IX PA6, 30% glass fiber/glass bead reinforced, impact modified, natural Information provided by Eurotec® |
|||
Melting Point | 223 °C | 433 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NB40 NL FA50 PA6, unfilled, flame retardant - halogen free, natural Information provided by Eurotec® |
|||
Melting Point | 223 °C | 433 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NB40 NL FN70 PA6, unfilled, flame retardant - halogen free (RoHS compliant), natural Information provided by Eurotec® |
|||
Melting Point | 223 °C | 433 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NB50 BK001 IH PA6, impact modified, black, extrusion grade Information provided by Eurotec® |
|||
Melting Point | 223 - 227 °C | 433 - 441 °F | DSC |
Gromax PBT 1100-211MB Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melting Point | 223 °C | 433 °F | ISO 11357-1/-2 |
BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled BK 15045 PBT Description: Easy flowing injection molding grade with 15 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg timer dials, toggles, knobs, parts for thermostats, oven-door .. |