Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Ultradur B 4300 G4 LS High Speed BK15045 20% Glass Filled PBT

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Manufacturer BASF
Trade Name Ultradur B
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF BASF Ultradur B 4300 G4 LS High Speed BK15045 20% Glass Filled PBT.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183
Melt Flow 28 g/10 min

@Load 2.16 kg,
Temperature 250 °C
28 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 115 MPa
16700 psi
5mm/min; ISO 527
Elongation at Break 3.0 %
3.0 %
5mm/min; ISO 527
Tensile Modulus 7.05 GPa
1020 ksi
1mm/min; ISO 527
Thermal Properties Metric English Comments
Melting Point 223 °C
433 °F
10 K/min
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ISO 75
Descriptive Properties Value Comments
Color BK15045
Commercial Status Active America
Impact Modified No
Primary Processing Technique Injection Molding