| Category | Polymer , Thermoplastic , Nylon , Nylon 6 |
| Manufacturer | PolyOne Corporation |
| Trade Name | Bergamid™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Bergamid™ B700 G20 H UF Polyamide 6 (Nylon 6).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.36 g/cc | 0.0491 lb/in³ | ±0.03 g/cm³; DIN 53479 |
| Ash | 20 % | 20 % | ISO 3451 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 95.0 MPa @Temperature 23.0 °C |
13800 psi @Temperature 73.4 °F |
ISO 527-2/5 |
| Elongation at Break | 2.1 % @Temperature 23.0 °C |
2.1 % @Temperature 73.4 °F |
ISO 527-2/5 |
| Tensile Modulus | 8.30 GPa @Temperature 23.0 °C |
1200 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
| Charpy Impact Unnotched | 5.30 J/cm² @Temperature 23.0 °C |
25.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
| Charpy Impact, Notched | 0.840 J/cm² @Temperature 23.0 °C |
4.00 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 223 °C | 433 °F | ISO 3146 |
| Maximum Service Temperature, Air | 110 °C | 230 °F | Continuous (GTP 50% Tensile); IEC 60216 |
| 190 °C | 374 °F | Short Time; IEC 60216 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | Unannealed; ISO 75-2/B |
| Flammability, UL94 | V-0 @Thickness 1.50 mm |
V-0 @Thickness 0.0591 in |
ALL; Internal Method |
| Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
0.8 mm wire; Ignition Temperature; IEC 60695-2-13 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
| Comparative Tracking Index | 600 V | 600 V | Solution A; IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Heat Stabilizer | |
| Features | Flame Retardant | |
| Halogen Free | ||
| Heat Stabilized | ||
| Low (to None) Phosphorus Content | ||
| Filler / Reinforcement | Glass Fiber Reinforcement, 20% Filler by Weight | |
| Forms | Pellets | |
| Generic Material | Nylon 6 | |
| Generic Name | Polyamide 6 (Nylon 6) | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| RoHS Compliance | RoHS Compliant |