Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 150 °C | 302 °F | STN EN 11357-1 |
Plastcom SLOVALEN PC 51 C 40 LS/1M Polypropylene reinforced with mineral filler, UV stabilized Modified copolymer PP for injection molding with the content of 40% mineral filler, UV stabilized. Product meets glow wire test at 750°C. Delivered in full RAL color scale.Information Provided by P.. |
|||
Melting Point | 150 °C | 302 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVALEN PC 51 T 20 Polypropylene Copolymer, 20% Micronized Talc FeaturesModified copolymer PP for injection moulding with the content of 20% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden f.. |
|||
Melting Point | 150 °C | 302 °F | |
Plastcom SLOVALEN PC 53 T 25 PP, 25% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 25% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Melting Point | 150 °C | 302 °F | |
Plastcom SLOVALEN PC 59 GB 10 PP, 10% glass beads FeaturesCompouded homopolymer PP, with the content of 10% chemically bound glass beads and modifier of mechanical properties. Increased strength in comparison with unfilled PP. Use in all industry s.. |
|||
Melting Point | 150 °C | 302 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVALEN PC 59 GF 13 Compounded Polypropylene Homopolymer, 13% Chemically Coupled Glass Fiber FeaturesCompounded homopolymer PP, with the content of 13% chemically coupled glass fiber and modifier of mechanical properties. Increased strength in comparison with unfilled PP. Use in all indus.. |
|||
Melting Point | 150 °C | 302 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVALEN PC 78 FRD 1 Polypropylene Copolymer, Halogen Flame Retardant, UV Stabilized FeaturesModified copolymer PP with the possibility of changing the MFI within the interval 5 - 20 g/10min. Stabilized against the UV-radiation by the UV stabilizer on the HALS basis. Retarded with.. |
|||
Melting Point | 150 °C | 302 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVALEN PC 78 FRD 3 Polypropylene Copolymer, Halogen Flame Retardant FeaturesDetermined for environment where contact with water is possible because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machine.. |
|||
Melting Point | 150 °C | 302 °F | |
Plastcom SLOVALEN PC 81 T 15 PP, 15% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 15% micronized, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitur.. |
|||
Melting Point | 150 °C | 302 °F | |
Plastcom SLOVALEN PC 81 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Melting Point | 150 °C | 302 °F | |
Plastcom SLOVALEN PC 82 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 30% micronized, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitur.. |
|||
Melting Point | 150 °C | 302 °F | |
Plastcom SLOVALEN PC 91 C 20 PP, 20% mineral filling FeaturesModified copolymer PP for injection moulding with the contenct of 20% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C depending on th.. |
|||
Melting Point | 150 °C | 302 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVALEN PH 51 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 130°C... |
|||
Melting Point | 150 °C | 302 °F | Flow temperature, ASTM D569-59 |
Rotuba 855, Slow Burning Ethyl Cellulose Data provided by the manufacturer. |
|||
Melting Point | 150 °C | 302 °F | DSC second heating; ASTM D3418 |
Reliance Industries Repol R019MZ Polypropylene REPOL Polypropylene R019MZ is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Melting Point | 150 °C | 302 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVALEN PC 53 N Polypropylene Copolymer, UV Stabilization FeaturesModified copolymer PP for injection moulding, with the ability of modeling the melt flow rate within the interval 5 - 20 g/10 min. Can be used for simple small as well as for large complica.. |
|||
Melting Point | 150 - 183 °C | 302 - 361 °F | Average value: 172 °C Grade Count:12 |
Overview of materials for Nylon 11, Flexible Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Flexible Tubing Grade". Each property range of values reported is minimum and maximum values o.. |
|||
Melting Point | 150 - 170 °C | 302 - 338 °F | ISO 3146-C |
FKuR Kunststoff Bio-Flex® F 6513 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Melting Point | 150 - 180 °C | 302 - 356 °F | ISO 3146-C |
FKuR Kunststoff Fibrolon® P 7550 Wood-Plastic Compound, Fiber Reinforced FIBROLON® are fiber reinforced compounds. Fibrolon® P 7550 has a polypropylene base. With the brand name of FIBROLON® FKuR has developed natural fiber reinforced compounds (Wood-Plastics-C.. |
|||
Melting Point | 150 °C | 302 °F | HS Method |
Hyosung Topilene C600 PP C600 Film Grade Butane Random CopolymerApplications: Metallizing CPPCharacteristics:Al bonding strengthHigh glossInformation provided by Hyosung Corporation |
|||
Melting Point | 150 - 160 °C | 302 - 320 °F | Kofler; MQSA 70 A |
Lubrizol Advanced Materials Pearlbond® DAP 750/2 Thermoplastic Polyurethane The Pearlbond® grades are aromatic crystalline TPUs used for the production of heat activated shoe counters and toe puffs, and orthopedic products. The Pearlbond® grades are supplied in pelle.. |
|||
Melting Point | 150 °C | 302 °F | ASTM D2117 |
SCG Chemicals EL-Proâ„¢ P851JO Polypropylene Injection Molding Key Characteristics:Good processabilityHigh gloss and brightnessOdorlessSafe for food contactRecommended Applications:Clear food containerClear large size containerThin wall productsInformation prov.. |
|||
Melting Point | 150 °C | 302 °F | ASTM D2117 |
SCG Chemicals EL-Proâ„¢ P852J Polypropylene Injection Molding Key Characteristics:Excellent productivityHigh clarityHigh stiffnessRecommended Applications:Clear food containerClear large size containerHousehold products and other articles that require high tra.. |
|||
Melting Point | 150 °C | 302 °F | DSC |
Total PPH M3661 Metallocene Isostatic Polypropylene Polymer, Cast Film Extrusion TOTAL Petrochemicals Polypropylene M3661 is an isostatic form of homopolymer made via TOTAL proprietary metallocene catalyst technologyRecommended Applications. M3661 is a medium molecular weight m.. |
|||
Melting Point | 150 °C | 302 °F | DSC |
Lubrizol ESTANE® ETE50DT3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Profile, Cable Jacket; Injection.. |
|||
Melting Point | 150 °C | 302 °F | Kofler |
Lubrizol Estane® MVT 70AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission Type: Estane® MVT 70AT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission with low water swell. Excellent low temperature properties and el.. |
|||
Melting Point | 150 °C | 302 °F | |
BASF Novolen® 3248 TC Polypropylene Easy-flowing grade containing nucleating and antistatic agents for transparent injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Melting Point | 150 °C | 302 °F | (Dry) |
Arkema Group Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11/xx,E,18-002Transparent and flexible copolymer for tubes extrusion. Additive free.High flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro.. |
|||
Melting Point | 150 °C | 302 °F | |
BASF Novolen® 3248 RC Polypropylene Grade containing nucleating and antistatic agents for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Melting Point | 150 - 170 °C | 302 - 338 °F | Average value: 164 °C Grade Count:14 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Melting Point | 150 - 300 °C | 302 - 572 °F | |
Johnson Matthey JM R-Core Soft Solder Flux A "rosin" type core generally used for joining copper and brass. Residues are non-corrosive.Information provided by Johnson Matthey. |