Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total PPH M3661 Metallocene Isostatic Polypropylene Polymer, Cast Film Extrusion

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Total Atofina
Trade Name PPH
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Total PPH M3661 Metallocene Isostatic Polypropylene Polymer, Cast Film Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TOTAL Petrochemicals Polypropylene M3661 is an isostatic form of homopolymer made via TOTAL proprietary metallocene catalyst technologyRecommended Applications. M3661 is a medium molecular weight material recommended for cast film extrusion. However, due to its unique and interesting properties, other applications may exist.FDA. M3661 complies with FDA regulations Title 21 CFR Section 177.1520 (c) 3.1and may be used under these provisions for food contact and packaging.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Melt Flow 14 g/10 min
14 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 810 %
810 %
ISO 527-3
Film Tensile Strength at Break, MD 40.0 MPa
5800 psi
ASTM D882
Film Tensile Strength at Break, TD 38.0 MPa
5510 psi
ASTM D882
1% Secant Modulus, MD 560 MPa
81200 psi
ASTM D882
1% Secant Modulus, TD 570 MPa
82700 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 150 °C
302 °F
DSC
Optical Properties Metric English Comments
Haze 0.40 %
0.40 %
ASTM D1003
Gloss 81 %
81 %
at 45°; ASTM D2457