Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 100 - 230 °C | 212 - 446 °F | Average value: 170 °C Grade Count:43 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Melting Point | 100 - 120 °C | 212 - 248 °F | MQSA 70 A |
Lubrizol Advanced Materials PEARLBOND® 115 Linear Thermoplastic Polyurethane
(discontinued **) PEARLBOND® 115 is a linear, aromatic polyurethane, supplied in form of white slightly yellowish pellets, which combines a very high crystallization rate with a high thermoplasticity level.Applicati.. |
|||
Melting Point | 100 °C | 212 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 3080 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 100 °C | 212 °F | DSC; ASTM D3418 |
DuPont™ Surlyn® 1652SBR Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating
(discontinued **) Surlyn® 1652SBR is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to pro.. |
|||
Melting Point | 100 °C | 212 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5020 400 Micron LDPE Powder Description: ICOFLO 510-5020 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melting Point | 100 °C | 212 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5052 1200 Micron LDPE Powder Description: ICOFLO 510-5052 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in m.. |
|||
Melting Point | 100 °C | 212 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5058 1200 Micron LDPE Powder Description: ICOFLO 510-5058 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melting Point | 100 °C | 212 °F | DSC; ASTM D3418 |
ICO Polymers ICOTEXâ„¢ 520-5019 300 Micron LDPE Powder Description: ICOTEX 520-5019 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and a .. |
|||
Melting Point | 100 °C | 212 °F | DSC; ASTM D3418 |
ICO Polymers ICOTEXâ„¢ 520-5050 500 Micron LDPE Powder Description: ICOTEX 520-5050 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and fa.. |
|||
Melting Point | 100 °C | 212 °F | DSC; ASTM D3418 |
ICO Polymers ICOTEXâ„¢ 520-5056 500 Micron LDPE Powder Description: ICOTEX 520-5056 is a low density polyethylene powder that has been developed to meet the special requirement of the textile coating industry. Key Characteristics: very high flow, very g.. |
|||
Melting Point | 100 °C | 212 °F | Eutectic |
Indium Corp. Indalloy 41 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 100 - 110 °C | 212 - 230 °F | MQSA 70 A |
Lubrizol Advanced Materials Pearlbond® DIPP-119 Thermoplastic Polyurethane Pearlbond™ DIPP-119 is polycaprolactone copolyester based thermoplastic polyurethane, supplied in form of translucent pellets. Featuring low melting point and excellent transparency, this produ.. |
|||
Melting Point | 100 °C | 212 °F | DSC; ASTM D3418 |
ICO Polymers ICOFLOâ„¢ 510-5064 1200 Micron LDPE Powder Description: ICOFLO 510-5064 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melting Point | 100 - 160 °C | 212 - 320 °F | |
Sibur AGG-G/B Atactic Polypropylene For preparation of polymer, bitumen-polymer and polymer-mineral mastics. Individual melts and compositions used for anti-corrosion covers for underground piping, different building structures, stru.. |
|||
Melting Point | 100 - 160 °C | 212 - 320 °F | |
Sibur APP-B Atactic Polypropylene For preparation of polymer, bitumen-polymer and polymer-mineral mastics. Individual melts and compositions used for anti-corrosion covers for underground piping, different building structures, stru.. |
|||
Melting Point | >= 100 °C | >= 212 °F | |
Struktol V-HCS Co-Stabilizing Processing Additive Blend fatty acid derived and functional inorganic materials.Applications: STRUKTOL® V-HCS is recommended for us with recycled rigid PVC where additional stabilization and lubrication is needed to.. |
|||
Melting Point | 100 °C | 212 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Nucrel® 910 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating 8.7 wt% Methacrylic Acid.Nucrel® 0910 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment de.. |
|||
Melting Point | 100 °C | 212 °F | Dow Method (DSC) |
Dow AFFINITY™ PL 1881G Polyolefin Plastomer (POP) AFFINITY™ PL 1881G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal products.In.. |
|||
Melting Point | 100 °C | 212 °F | DSC, 10°C/min; DuPont Test |
Dow Engage® 8480 Polyolefin Elastomer Description: Engage® 8480 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in footwear applications and profile extrusion of tubing and hoses. It has good clari.. |
|||
Melting Point | 100 °C | 212 °F | D.S.C. method |
Arkema Group Orevac® 9309 Film EVA-MAH Terpolymer EVA Terpolymers based Main Application: Cast film coextrusionInformation provided by Arkema Group |
|||
Melting Point | 100 °C | 212 °F | |
AIM 35.7Sn/35.7Pb/28.6Bi Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Melting Point | 100 - 140 °C | 212 - 284 °F | Average value: 107 °C Grade Count:26 |
Overview of materials for Low Density Polyethylene (LDPE), Masterbatch Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Masterbatch Grade". Each property range of values reported is minimum a.. |
|||
Melting Point | 100 °C | 212 °F | DSC; ASTM D3418 |
DuPont™ Surlyn® 1652SR Zinc Ionomer Resin for Cast Film and Extrusion Coating Surlyn® 1652SR is an ionomer resin available for use in cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene resi.. |