Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Nucrel® 910 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating

Category Polymer , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Coating Grade
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Nucrel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Nucrel® 910 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
8.7 wt% Methacrylic Acid.Nucrel® 0910 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethylene resins.Features/Benefits vs. Nucrel® 0609HS: Better adhesion to unprimed foil, paper and metallized film provides better substrate protection, improved structure reliability, and barrier integrity. This product provides good, but lower adhesion to PE. Lower seal initiation temperature allows higher speed packaging. Better hot tack, sealability through contamination, and heat seal strength provides stronger, more reliable heat seals.Typical Applications: Foil-containing shampoo, toothpaste, towelette, condiment and miscellaneous non-food pouches and sachets; Medical/pharmaceutical packaging; Snack structures; Toothpaste tubes; Cable shield wrap; Aseptic and hot-fill liquid cartons; Other foil, metallized film, or paper coatings as a heat seal or tie layer.Information provided by DuPont Packaging Polymers.
Physical Properties Metric English Comments
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Seal Strength 1300 g/25 mm
1300 g/in
seal bar 110°C.
Hot Tack Strength 1150 g/25 mm
1150 g/in
seal bar 102°C; Packforsk method.
Thermal Properties Metric English Comments
Melting Point 82.0 °C
180 °F
Freezing Point via DSC/ASTM D3418
100 °C
212 °F
Upon Melting via DSC/ASTM D3418
Vicat Softening Point 81.0 °C
178 °F
ASTM D1525
Processing Properties Metric English Comments
Nozzle Temperature 305 °C
581 °F
Typical Die Temp.
Melt Temperature 260 - 305 °C
500 - 581 °F
Copyright © lookpolymers.com All Rights Reserved