Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 80.0 °C | 176 °F | |
Omnia Plastica PVC Polyvinylchloride A widely used material, its application is under regulation in many countries for ecological reasons and it is often substituted by PP or other polymers. It is chosen for its chemical resistance.Fea.. |
|||
Melting Point | 80.0 °C | 176 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Bynel® 11E573 Modified EVA Adhesive Resin
(discontinued **) Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Melting Point | 80.0 °C | 176 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 3048 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 80.0 - 110 °C | 176 - 230 °F | TMA Melt Range |
Huntsman IROGRAN® CA116-203 TPU-Polyester Introduction: IROGRAN CA116-203 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-203 is part of the HUNTSMAN film and shee.. |
|||
Melting Point | 80.0 - 110 °C | 176 - 230 °F | TMA Melt Range |
Huntsman IROGRAN® CA116-205 TPU-Polyester Introduction: IROGRAN CA116-205 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-205 is part of the HUNTSMAN film and shee.. |
|||
Melting Point | 80.0 - 88.0 °C | 176 - 190 °F | |
M Chemical GUARD DOGâ„¢ UV328 Benzotriazole UV Absorber GUARD DOGâ„¢ UV328 light stabilizer is a derivative of Benzotriazole that has exceptionally strong and broad-range UV absorption properties throughout the UV spectrum specially designed for polym.. |
|||
Melting Point | 80.0 - 86.0 °C | 176 - 187 °F | |
M Chemical GUARD DOGâ„¢ UV770 HALS Light Stabilizer GUARD DOGâ„¢ UV770 unhindered amine light stabilizer is a highly effective radical scavenger that protects polymers against degradation caused by exposure to UV radiation.Applications: Extremely.. |
|||
Melting Point | 80.0 - 89.0 °C | 176 - 192 °F | |
Indium Corp. Indalloy 31 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 80.0 °C | 176 °F | TMA; MCI Method |
Mitsui APELâ„¢ APL8008T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Melting Point | 80.0 - 84.0 °C | 176 - 183 °F | MQSA 70 A |
Lubrizol Advanced Materials Pearlbond® ECO D590 Thermoplastic Polyurethane Pearlbond™ ECO D590 is a linear, aromatic bio-polyurethane based on specialty polyol from renewable sources, supplied in form of white spherical granules, with an extremely high crystallization.. |
|||
Melting Point | 80.0 - 85.0 °C | 176 - 185 °F | MQSA 70 A |
Lubrizol Advanced Materials Pearlbond® Eco D900 Thermoplastic Polyurethane Pearlbond™ ECO D900 is a linear, aromatic polyurethane based on specialty polyol from renewable sources. It contains 67% of renewable material as certified according to ASTM-D6866. It is suppli.. |
|||
Melting Point | 80.0 °C | 176 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Nucrel® 31001 Ethylene-Acrylic Acid Copolymer Resin for Blown and Cast Film 9.5 wt% Acrylic Acid.Nucrel® 31001 is an ethylene-acrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins.F.. |
|||
Melting Point | 80.0 - 94.0 °C | 176 - 201 °F | ASTM D3418(DSC) |
DuPont Nucrel® 699 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Melting Point | 80.0 °C | 176 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 3861 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 80.0 °C | 176 °F | Freezing Point, DSC; ASTM D3418 |
DuPont Nucrel® AE High Performance Adhesive and Sealant Resin Nucrel® Nucrel® AE is a terpolymer of ethylene, methacrylic acid, and acrylate, available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designe.. |
|||
Melting Point | 80.0 °C | 176 °F | DSC |
Arkema Group LOTRYL® 20 MA 08 Copolymer Ethylene - Methyl Acrylate LOTRYL® 20 MA 08 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 20 MA 08 is a polyme.. |
|||
Melting Point | 80.0 °C | 176 °F | D.S.C. method |
Arkema Group Orevac® 18216 Maleic Anhydride modified EVA Orevac® 18216 resin is a maleic anhydride modified ethylene - vinyl acetate copolymer designed for the coextrusion of multilayer barrier structures providing outstanding adhesion between layers.Inf.. |
|||
Melting Point | 80.0 °C | 176 °F | DSC |
Arkema Group OREVAC® 9304 EVA Terpolymer OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre.. |
|||
Melting Point | 80.0 °C | 176 °F | |
C.O.I.M. UREXTER® F 3 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |
|||
Melting Point | 80.0 °C | 176 °F | |
C.O.I.M. UREXTER® Lp 2500_30 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |
|||
Melting Point | 80.0 °C | 176 °F | |
C.O.I.M. UREXTER® Lp 285 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |
|||
Melting Point | 80.0 °C | 176 °F | |
C.O.I.M. UREXTER® T 400 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |
|||
Melting Point | 80.0 °C | 176 °F | |
C.O.I.M. UREXTER® T 404 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |
|||
Melting Point | 80.0 °C | 176 °F | DSC |
Arkema Group LOTADER® 4503 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 4503 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process.LOTADER 4503 is a versatile adhesive for extrusion lamination, des.. |
|||
Melting Point | 80.0 °C | 176 °F | DSC |
Arkema Group LOTADER® 5500 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 5500 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure autoclave process. These grade is characterised by a high fluidity. Functional group.. |
|||
Melting Point | 80.0 °C | 176 °F | DSC |
Arkema Group LOTRYL® 20 MBG 08 Copolymer Ethylene - Methyl Acrylate LOTRYL® 20MBG08 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 20 MBG 08 is a polyme.. |
|||
Melting Point | 80.0 °C | 176 °F | |
M. Holland Company MAGMA® LM311-D LLDPE
(discontinued **) Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland. |
|||
Melting Point | >= 80.0 °C | >= 176 °F | AM6512 |
Solvay RHODAPHOSE® TRIPHENYL PHOSPHINE Phosphorus Derivative Identification: TRIPHENYLPHOSPHINECAS: 603 – 35 – 0Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: TRIPHENYL PHOSPHINE is an intermediate for use as a phase transf.. |