Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 870 °C | 1600 °F | |
Mateck Lithium Fluoride (LiF) Optical crystals |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 165 Forgings & Extrusions; AT (TF00) Temper (UNS C17000) Treatment required for max strength: 3 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; AT (TF00) Temper; All Thicknesses (UNS C17000) Treatment required for max strength: 3 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; H (TD04) Temper; over 9.5 to 25 mm Thickness (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 165 Rod and Bar; AT (TF00) Temper; over 76 mm (UNS C17000) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 190 Strip; XHMS (TM08) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 69%Formability Ratio, 90° Bend, R.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Forgings & Extrusions; AT (TF00) Temper (UNS C17200) Treatment required for max strength: 3 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; AT (TF00) Temper; All Thicknesses (UNS C17200) Treatment required for max strength: 3 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; H (TD04) Temper; over 9.5 to 25 mm Thickness (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; H (TD04) Temper; up to 9.5 mm Thickness (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 9.5 to 25 mm Thickness (UNS C17200) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Rod and Bar; A (TB00) Temper; All Sizes (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Strip; A -Dead Soft (TB00) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): 0Superficial Hardness: 30T 46-67Tabulated properties apply .. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Strip; AT (TF00) Temper (UNS C17200) Treatment required for max strength: 3 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 70%Superficial Hardness: 30N 56-6.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Strip; H (TD04) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 1Formability Ratio (bad Way): 2.9Superficial Hardness: 30T 79-83Tabulated properties appl.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Strip; HT (TH04) Temper (UNS C17200) Treatment required for max strength: 2 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 74%Superficial Hardness: 30N 58-6.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Tube; AT (TF00) Temper; over 76 mm o.d. (UNS C17200) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Wire; 1/4H (TD01) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Wire; 1/4HT (TH01) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: 2 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed i.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: 3 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed i.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy M25 Rod and Bar; HT (TH04) Temper; over 9.5 to 25.4 mm (UNS C17300) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy M25 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: 3 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed i.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM00 Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 76%Formability Ratio, 90° Bend, R.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM02 Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 76%Formability Ratio, 90° Bend, R.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM04 Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 77%Formability Ratio, 90° Bend, R.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM08 Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation after 1000 hrs @ 200°C: 78%Formability Ratio, 90° Bend, R.. |
|||
Melting Point | 871 °C | 1600 °F | |
Heatbath/Park High Speed 60 High Speed Hardening Salt Solution Treating Salt. A neutral salt designed for heat treatment high alloy steels requiring temperatures of 1650° to 2200°F. Formulated per MIL-S-10699-B, Class 6.Information provided by H.. |
|||
Melting Point | 870 - 980 °C | 1600 - 1800 °F | |
Materion Beryllium Copper Alloy 25 Wire; 1/2HT (TH02) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: 1.5 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed.. |
|||
Melting Point | 870 - 930 °C | 1600 - 1710 °F | |
Wieland 1410 Wilaform Gold Yield alloy. Particularly suitable for the production of strongly deformed or thick chains.Applications: casting, chains, coin/shapeDental |