Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
Murtfeldt Material ”S”® 1000 Green Polyethylene Material ”S”® 1000 is exclusively produced from ultra-high molecular weight polyethylene powder that is mixed with finely milled Original Material ”S”®. The fine milled material is compressio.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
Murtfeldt Material ”S”® 1000 RB Polyethylene, High Friction An elastomer in Material ”S”® 1000 RB gives it high impact resistance and skid resistance.Special Properties:• High coefficient of friction• Good wear and abrasion resistanceInformation provide.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
Murtfeldt Original Material ”S”® Black Antistatic Polyethylene, Conductive Original Material ”S”® black has the same properties as Original Material ”S”® green/natural. In addition, it is also electrostatically conductive due to the addition of additives. Special Pro.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
Murtfeldt Original Material ”S”® Green Polyethylene Material ”S”® is based on virgin, ultrahigh molecular weight low pressure polyethylene and significantly exceeds the requirements of DIN 16972. In particular, Material ”S”® green has excellen.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
Murtfeldt Original Material ”S”® plus + ESD Polyethylene, Conductive Material ”S”® plus+ ESD has extremely low electrical resistance and is an optimum conductor. Full voltage dissipation for earthed components at maximum speed enables safe, spark-free work. This m.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
Murtfeldt Original Material ”S”® plus + LF Polyethylene, Low Friction This material has half the sliding friction coefficient of the Original Material ”S”®. This enables an increased machine running speed at the same time as less abrasion and thus a lower maintenan.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
Murtfeldt Original Material ”S”® plus + TLS Polyethylene Original Material ”S”® plus+ TLS is designed for high temperature industrial applications for which Original Material ”S”® could previously not be used. The thermal oxidation point has been i.. |
|||
Melting Point | 133 - 135 °C | 271 - 275 °F | DSC ISO 3146 |
Okulen® 1000 - REG PE Colored OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Melting Point | 133 - 135 °C | 271 - 275 °F | DSC ISO 3146 |
Okulen® 1000 PE-UHMW, AST OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | DSC ISO 3146 |
Okulen® 500 - REG PE Colored OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | DSC ISO 3146 |
Okulen® 500 - REG PE Multicoloured coarse OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | DSC ISO 3146 |
Okulen® 500 - REG PE Multicoloured fine OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | DSC ISO 3146 |
Okulen® 500 PE-HMW, AST OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | DSC ISO 3146 |
Okulen® 500 PE-HMW, UV - stabilized OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Melting Point | 125 - 135 °C | 257 - 275 °F | ASTM D3418 |
NatureWorks® Ingeo™ 6060D Fiber Grade PLA NatureWorks PLA polymer 6060D is an amorphous thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6060D is designed for extrusion into mech.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146; DSC, 10°C/min |
Quadrant EPP Cesticolor™ HD 500 Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146; DSC, 10°C/min |
Quadrant EPP Cestilene™ HD 1000 R Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146; DSC, 10°C/min |
Quadrant EPP Cestilene™ HD 500 Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146; DSC, 10°C/min |
Quadrant EPP Cestilene™ HD 500 R Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Melting Point | 72.0 - 135 °C | 162 - 275 °F | Average value: 127 °C Grade Count:49 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Melting Point | 100 - 135 °C | 212 - 275 °F | |
M Chemical GUARD DOGâ„¢ UV944 HALS Light Stabilizer GUARD DOGâ„¢ UV944 hindered amine light stabilizer is a highly effective radical scavenger that protects polymers against degradation caused by exposure to UV radiation. It is an oligomeric HALS.. |
|||
Melting Point | 96.0 - 135 °C | 205 - 275 °F | |
Indium Corp. Indalloy 74 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | Crystalline melting range |
Mikro-Technik Mikrolen UHMW-PE Properties: very good impact resistance / high absorption at shock and impact stress extremely high resistance against abrasive wear good corrosion resistance highly resistant at temperatures of -26.. |
|||
Melting Point | 120 - 135 °C | 248 - 275 °F | |
DayGlo ZQ Pigments ZQ-11 Aurora Pink DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Melting Point | 120 - 135 °C | 248 - 275 °F | |
DayGlo ZQ Pigments ZQ-13 Rocket Red DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Melting Point | 120 - 135 °C | 248 - 275 °F | |
DayGlo ZQ Pigments ZQ-16 Arc Yellow DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Melting Point | 120 - 135 °C | 248 - 275 °F | |
DayGlo ZQ Pigments ZQ-21 Corona Magenta DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | DIN 53 736 |
Hippe PE 1000 Polyethylene Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | DIN 53 736 |
Hippe PE 500 Polyethylene Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | 10K/min; ISO 3146 |
CENTROPLAST CENTROLEN PE-HD Polyethylene high density This material is a low density, easily machined plastic that can be welded and has good chemical resistance. Applications include apparatus engineering, and machines in the foodstuff industry.Infor.. |