Mikro-Technik Mikrolen UHMW-PE

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Ultra High Molecular Weight
Manufacturer Mikro-Technik
Trade Name Mikrolen
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mikro-Technik Mikrolen UHMW-PE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Properties: very good impact resistance / high absorption at shock and impact stress extremely high resistance against abrasive wear good corrosion resistance highly resistant at temperatures of -265°C up to +80°C (100°C) in relation to mechanical stressInformation provided by Mikro-Technik GmbH
Physical Properties Metric English Comments
Density >= 0.930 g/cc
>= 0.0336 lb/in³
Molecular Weight 7.60e+6 g/mol
7.60e+6 g/mol
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
15 sec
61
61
3 sec
Ball Indentation Hardness 36.0 MPa
5220 psi
30 sec
Tensile Strength, Yield >= 40.0 MPa
>= 5800 psi
Elongation at Break >= 350 %
>= 350 %
Izod Impact, Notched (ISO) >= 130 kJ/m²
>= 61.9 ft-lb/in²
double notch
NB
NB
single notch
Thermal Properties Metric English Comments
CTE, linear 200 µm/m-°C

@Temperature 23.0 - 80.0 °C
111 µin/in-°F

@Temperature 73.4 - 176 °F
Thermal Conductivity 0.410 W/m-K
2.85 BTU-in/hr-ft²-°F
Melting Point 130 - 135 °C
266 - 275 °F
Crystalline melting range
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
Surface Resistance >= 1.00e+11 ohm
>= 1.00e+11 ohm
Dielectric Strength 45.0 kV/mm
1140 kV/in
Descriptive Properties Value Comments
Tensile E-modulus 6.8