Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Murtfeldt Original Material ”S”® plus + ESD Polyethylene, Conductive

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer Murtfeldt Kunststoffe GmbH & Co
Trade Name Original Material ”S”®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Murtfeldt Original Material ”S”® plus + ESD Polyethylene, Conductive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material ”S”® plus+ ESD has extremely low electrical resistance and is an optimum conductor. Full voltage dissipation for earthed components at maximum speed enables safe, spark-free work. This material provides a cost-effective alternative to carbon-filled PTFE.Special Properties:• Very good conductivity• Voltage dissipation on surface in less than 0.1s• Suitable for devices and machines subject to Directive 94/9/EC (ATEX 95) • Approved for use in the food industry (EU and FDA)Information provided by Murtfeldt Kunststoffe GmbH & Co. KG.
Physical Properties Metric English Comments
Density <= 0.930 g/cc
<= 0.0336 lb/in³
ISO 1183
Moisture Absorption at Equilibrium <= 0.10 %
<= 0.10 %
ISO 62
Water Absorption at Saturation <= 0.10 %
<= 0.10 %
ISO 62
Molecular Weight 5.00e+6 g/mol
5.00e+6 g/mol
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
DIN 53505
Ball Indentation Hardness 38.0 MPa
5510 psi
Tensile Strength at Break 25.0 MPa
3630 psi
ISO 527
Tensile Strength 20.4 MPa
2960 psi
ISO 527
Tensile Strength, Yield >= 20.0 MPa
>= 2900 psi
ISO 527
Elongation at Break 290 %
290 %
ISO 527
Modulus of Elasticity 0.750 GPa
109 ksi
Compressive Yield Strength 6.00 MPa

@Strain 1.00 %
870 psi

@Strain 1.00 %
ISO 604
10.5 MPa

@Strain 2.00 %
1520 psi

@Strain 2.00 %
ISO 604
18.0 MPa

@Strain 5.00 %
2610 psi

@Strain 5.00 %
ISO 604
Charpy Impact, Notched >= 12.0 J/cm²
>= 57.1 ft-lb/in²
ISO 179
Coefficient of Friction, Dynamic 0.10 - 0.20
0.10 - 0.20
Sand Slurry 110
110
value in %
Thermal Properties Metric English Comments
CTE, linear 200 µm/m-°C

@Temperature 23.0 - 60.0 °C
111 µin/in-°F

@Temperature 73.4 - 140 °F
Thermal Conductivity 0.400 W/m-K
2.78 BTU-in/hr-ft²-°F
ISO 52612
Melting Point 130 - 135 °C
266 - 275 °F
ISO 3146
Maximum Service Temperature, Air 90.0 °C
194 °F
Short Term
80.0 °C

@Time 1.80e+7 sec
176 °F

@Time 5000 hour
Minimum Service Temperature, Air -150 °C
-238 °F
Glass Transition Temp, Tg -120 °C
-184 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Electrical Resistivity <= 10000 ohm-cm
<= 10000 ohm-cm
IEC 60093
Surface Resistance <= 10000 ohm
<= 10000 ohm
IEC 60093
Compliance Properties Metric English Comments
FDA Yes
Yes
Descriptive Properties Value Comments
Color Black