Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 320 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 320 - 330 °C
608 - 626 °F
ISO 11357-3
PolyOne Edgetek® AM-35GF/000 FR NH Polyphthalamide (PPA)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Melting Point 320 - 325 °C
608 - 617 °F
Solvay Specialty Polymers Polymist® F-5 PTFE Powder Lubricant  (discontinued **)
Polymist® powders are a family of white free-flowing polytetrafluoroethylene powders for use as additives in other materials to enhance processing or end-use performance characteristics. Polymist ..
Melting Point 320 - 325 °C
608 - 617 °F
Solvay Specialty Polymers Polymist® F-5A PTFE Powder Lubricant  (Unverified Data**)
Polymist® powders are a family of white free-flowing polytetrafluoroethylene powders for use as additives in other materials to enhance processing or end-use performance characteristics. Polymist ..
Melting Point 320 - 340 °C
608 - 644 °F
Melting Range; DTA
Fluorseals PTFE Unfilled
Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.
Melting Point 320 °C
608 °F
Mitsui Arlenâ„¢ A315 15% Glass Fiber-Reinforced Modified Nylon 6T (COND)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss..
Melting Point 320 °C
608 °F
Mitsui Arlenâ„¢ A315 15% Glass Fiber-Reinforced Modified Nylon 6T (DAM)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss..
Melting Point 320 °C
608 °F
Mitsui Arlenâ„¢ A335 35% Glass Fiber-Reinforced Modified Nylon 6T (DAM)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss..
Melting Point 320 °C
608 °F
Mitsui Arlenâ„¢ A350 50% Glass Fiber-Reinforced Modified Nylon 6T (DAM)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss..
Melting Point 320 - 330 °C
608 - 626 °F
ASTM D3418
Solvay Specialty Polymers Algoflon® L600 Polytetrafluoroethylene (PTFE)
Algoflon® L600 a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles. Algoflon® L600 can be de-agglomerated..
Melting Point 320 °C
608 °F
Dry; ISO 11357-3
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned)
Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera..
Melting Point 320 °C
608 °F
ISO 11357-3
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera..
Melting Point 320 °C
608 °F
DSC
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera..
Melting Point 320 - 330 °C
608 - 626 °F
ASTM-D-4591
Shamrock Technologies Fluoro FR-150 Anti-dripping Thermoplastic Grade PTFE Additive
The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins (and to polymeric resins containing glass fiber) provides greatly increased resistance to surface wear and abrasi..
Melting Point 320 - 330 °C
608 - 626 °F
ASTM-D-4591
Shamrock Technologies Fluoro T® 702 Thermoplastic Grade PTFE Additive
The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction ..
Melting Point 320 - 330 °C
608 - 626 °F
ASTM-D-4591
Shamrock Technologies Fluoro T® 707 Thermoplastic Grade PTFE Additive
The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction ..
Melting Point 320 - 330 °C
608 - 626 °F
ASTM-D-4591
Shamrock Technologies Fluoro T® 715 Thermoplastic Grade PTFE Additive
The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction ..
Melting Point 320 - 330 °C
608 - 626 °F
ASTM-D-4591
Shamrock Technologies Fluoro T® 802 Thermoplastic Grade PTFE Additive
The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction ..
Melting Point 320 - 330 °C
608 - 626 °F
ASTM-D-4591
Shamrock Technologies Fluoro T® 811 Thermoplastic Grade PTFE Additive
The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction ..
Melting Point 320 - 330 °C
608 - 626 °F
ASTM-D-4591
Shamrock Technologies MicroFLON® 1253 Thermoplastic Grade PTFE Additive
Special grade for fine dispersion.The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a..
Melting Point 320 - 330 °C
608 - 626 °F
ASTM-D-4591
Shamrock Technologies Fluoro T® 602 Thermoplastic Grade PTFE Additive
The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction ..
Melting Point 320 - 330 °C
608 - 626 °F
ASTM-D-4591
Shamrock Technologies Fluoro T® 611 Thermoplastic Grade PTFE Additive
The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction ..
Melting Point 320 °C
608 °F
DSC
Wolf Kunststoff ZEDEX® ZX-410 A4A Polymer Alloy
ZX-410 is a bearing material with excellent properties and a very affordable price.Main Characteristics: Hard, Stiff, Tough; High dimensional stability; High chemical resistance; High water resistan..
Melting Point 320 °C
608 °F
DSC
Wolf Kunststoff ZEDEX® ZX-530 A5D Polymer Alloy
Main Characteristics: Low Creep; Low moisture absorption; Flame retardant; Low impurity ions; Good machinability; FDA compliant LABS; Extremely low outgassing; Less expensive than PEEK; Stress resis..
Melting Point 320 °C
608 °F
DSC
Wolf Kunststoff ZEDEX® ZX-530CD3 031 Polymer Alloy, Fiber Reinforced and PTFE Modified
Main Characteristics: Dimensionally stable and rigid; Stress resistant; Extremely low wear to 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsIn..
Melting Point 320 °C
608 °F
ISO 3149
ExxonMobil PP1013H1 Polypropylene Homopolymer
Product Description: A homopolymer resin that meets certified requirements for use in Medical and Pharmaceutical applications.Availability: Europe and North America Features:Autoclave SterilizableE..
Melting Point 320 °C
608 °F
ISO 3146
ExxonMobil PP1063L1 Polypropylene Homopolymer
Product Description: A homopolymer resin designed for general use. It is suitable for masterbatch carrier and other compounding applications and for the molding of caps, cups, containers and other ..
Melting Point 320 °C
608 °F
Mitsui Arlen™ AE4200 Modified Nylon 6T, for Tribolic Applications (DAM)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it possesses ..
Melting Point 320 °C
608 °F
ISO 11357-3
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature..
Copyright © lookpolymers.com All Rights Reserved