Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 300 - 323 °C | 572 - 613 °F | Average value: 313 °C Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Melting Point | 300 °C | 572 °F | 10°C/min, First Heat; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® HTN 51G15HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G15HSL BK083 is a 15% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |
|||
Melting Point | 300 °C | 572 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, Dry as Molded
(discontinued **) AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properti.. |
|||
Melting Point | 300 °C | 572 °F | ASTM D3418 |
Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, Dry as Molded
(discontinued **) AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properti.. |
|||
Melting Point | 300 °C | 572 °F | ASTM D3418 |
Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, at 50% RH
(discontinued **) AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properti.. |
|||
Melting Point | >= 300 °C | >= 572 °F | |
Solvay Specialty Polymers Hyflon® PFA 450 Fluoropolymer
(discontinued **) Data provided by the manufacturer.Hyflon® PFA 450 has outstanding physical and chemical properties typical of fluoropolymers.Hyflon® PFA 420 |
|||
Melting Point | 300 - 315 °C | 572 - 599 °F | Average value: 307 °C Grade Count:16 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
Melting Point | 300 - 320 °C | 572 - 608 °F | |
Indium Corp. Indalloy 168 Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 300 - 310 °C | 572 - 590 °F | |
Indium Corp. Indalloy® 164 Pb-In-Ag Solder Alloy This alloy is very useful in the 300°C range. It has particularly good thermal fatigue properties as well as the minimal gold leaching properties of indium-lead alloys. Often used in reducing atm.. |
|||
Melting Point | 300 °C | 572 °F | 10°C/min; ISO 11357-1/-3 |
Kuraray Genestarâ„¢ G1350A-M42 Nylon, 35% Glass Filled 35% Glass reinforced injection grade. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment.Main Features:Hydrolysis resistanceHeat resista.. |
|||
Melting Point | 300 °C | 572 °F | 10°C/min; ISO 11357-1/-3 |
Kuraray Genestarâ„¢ G1352A-M41 Nylon, 35% Glass Filled Low friction reinforced injection grade.Main Features:Low friction coefficientAbrasion resistanceExamples of applications:Friction and wear applicationGear and wheel |
|||
Melting Point | 300 °C | 572 °F | 10°C/min; ISO 11357-1/-3 |
Kuraray Genestarâ„¢ G1500A-M61 Nylon, 50% Glass Filled 50% Glass reinforced injection grade. Main Features:High strengthHeat resistanceExamples of applications:Structural partsSteel alternating parts |
|||
Melting Point | 300 °C | 572 °F | 10°C/min; ISO 11357-1/-3 |
Kuraray Genestarâ„¢ GX1500A-M41 Nylon, 50% Glass Filled 50% Glass reinforced injection grade. This grade was developed specifically for high mechanical properties for TD direction.Main Features:Low warpageHigh mechanical properties for TD directionExamp.. |
|||
Melting Point | 300 °C | 572 °F | 10°C/min; ISO 11357-1/-3 |
Kuraray Genestarâ„¢ N1000A-M41 Nylon Standard unreinforced injection grade. Main features:Low water absorptionChemical ResistanceExamples of application are:Friction and wear applicationGear and Wheel |
|||
Melting Point | 300 °C | 572 °F | 10°C/min; ISO 11357-1/-3 |
Kuraray Genestarâ„¢ N1001A-M41 Nylon Low friction unreinforced injection grade. Main Features:Low friction coefficientHigh impact strengthExamples of applications are:Friction and wear applicationGear and wheel |
|||
Melting Point | 300 °C | 572 °F | 10°C/min; ISO 11357-1/-3 |
Kuraray Genestarâ„¢ N1002A-M41 Nylon Low friction unreinforced injection grade. Main Features:Low friction coefficientLow wearExamples of applications are:Friction and wear applicationGear and wheel |
|||
Melting Point | 300 °C | 572 °F | 10°C/min; ISO 11357-1/-3 |
Kuraray Genestarâ„¢ N1006A-M41 Nylon Impact modified unreinforced injection grade. Main Features:High elongationHigh impact strengthExamples of applications are:Retainers for quick connectorFlexible band |
|||
Melting Point | 300 - 310 °C | 572 - 590 °F | DSC |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Melting Point | 300 - 310 °C | 572 - 590 °F | DSC |
Solvay Specialty Polymers Hyflon® PFA P7310 Perfluoroalkoxy (PFA) Hyflon® PFA P7310 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in anti.. |
|||
Melting Point | 300 - 310 °C | 572 - 590 °F | DSC |
Solvay Specialty Polymers Hyflon® PFA P7010 Perfluoroalkoxy (PFA) Hyflon® PFA P7010 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in anti.. |
|||
Melting Point | 300 - 314 °C | 572 - 597 °F | |
Williams Advanced Alloys WS314 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 300 °C | 572 °F | DAM; first heat; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® HTN 51G15HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 15% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G15HSL BK083 is a 15% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
Melting Point | 300 °C | 572 °F | DAM; first heat; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G45HSL BK083 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
Melting Point | 300 °C | 572 °F | DAM; first heat; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® HTN FE8200 BK431 Polyphthalamide (PPA)
(Unverified Data**) Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 BK431 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also.. |
|||
Melting Point | 300 °C | 572 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® XE 4217 black 9233 PA6T/66-GF45 Product description: Grivory XE 4217 black 9233 is a high heat stabilized, 45% glass fiber reinforced, semicrystalline, thermoplastic engineering material for injection moulding. Polymer designation.. |
|||
Melting Point | >= 300 °C | >= 572 °F | |
BASF LUMOGEN® 570 F Violet Type of Dye: PeryleneNote on Fastness to Weathering: 0.02% in PMMA injection-molded plaques of 2 mm thickness Residual fluorescence(%) after 80 days accelerated exposure in Xenotest 1200Color Index:.. |
|||
Melting Point | >= 300 °C | >= 572 °F | |
BASF LUMOGEN® 240 F Orange Type of Dye: PeryleneNote on Fastness to Weathering: 0.02% in PMMA injection-molded plaques of 2 mm thickness Residual fluorescence(%) after 80 days accelerated exposure in Xenotest 1200Information .. |
|||
Melting Point | 300 - 310 °C | 572 - 590 °F | ASTM D3307 |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Melting Point | 300 °C | 572 °F | 10°C/min, First Heat; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |