Solvay Specialty Polymers Hyflon® PFA P7010 Perfluoroalkoxy (PFA)

Category Polymer , Thermoplastic , Fluoropolymer , PFA
Manufacturer Solvay Specialty Polymers
Trade Name Hyflon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Hyflon® PFA P7010 Perfluoroalkoxy (PFA).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Hyflon® PFA P7010 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in antistick applications. Hyflon® PFA P7010 exhibits very low surface energy, very low coefficient of friction and excellent thermal and flame resistance Additionally Hyflon® PFA P7010 coatings show excellent smooth surface finish, outstanding antistick behavior and can maintain performance over a wide temperature range.Features: Good Surface Finish; Good Thermal Stability; Low Friction; Semi CrystallineUses: Coating ApplicationsAdditional Properties: Average Particle Size - Internal Method 25 µmInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 2.16 g/cc
0.0780 lb/in³
ASTM D792
Melt Flow 10 - 17 g/10 min

@Load 5.00 kg,
Temperature 372 °C
10 - 17 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 300 - 310 °C
572 - 590 °F
DSC
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Clear/Transparent
Form Powder
Processing Technique Coating
Users viewing this material also viewed the following: