Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 223 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 223 °C
433 °F
Nylacast Moly Cast Nylon 6, MoS2 Filled
Nylacast Moly is part of the Cast Nylon 6 family. Its improved crystallization occurs by the addition of Molybdenum Disulphide. It includes MoS2, which is an extremely effective self dry lubricant w..
Melting Point 223 °C
433 °F
ISO 3146
PolyOne Bergamid™ B65 G30 black IG Polyamide 6 (Nylon 6)
Information provided by PolyOne
Melting Point 223 °C
433 °F
ISO 3146
PolyOne Bergamid™ B650 G/Mi20 UF Polyamide 6 (Nylon 6)
Information provided by PolyOne
Melting Point 223 °C
433 °F
ISO 3146
PolyOne Bergamid™ B700 G20 H UF Polyamide 6 (Nylon 6)
Information provided by PolyOne
Melting Point 223 °C
433 °F
ISO 3146
PolyOne Bergamid™ B700 UF Polyamide 6 (Nylon 6)
Information provided by PolyOne
Melting Point 223 °C
433 °F
DSC Peak; JIS K7121
Goodfellow TPX® DX310 Coating/Extrusion Grade Polymethylpentene
This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a..
Melting Point 223 °C
433 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Crastin® CE15315 BK010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin CE15315 BK010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0..
Melting Point 223 °C
433 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Crastin® FGS600F10 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced Polybutylene Terephthalate Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Melting Point 223 °C
433 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Crastin® S600F10 BK851 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin S600F10 BK851 is an unreinforced lubricated medium high viscosity black polybutylene tere..
Melting Point 223 °C
433 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Crastin® S610SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)<
Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin S610SF is an unreinforced low viscosity polybutylene terephthalate for injection molding. It has hig..
Melting Point 223 °C
433 °F
10 K/min; ISO 3146
Eurotec® Tecomid® NB40 GR40 NL PA 6 40% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Melting Point 223 °C
433 °F
10 K/min; ISO 3146
Eurotec® Tecomid® NB40 NL IH PA 6 impact modified
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Melting Point 223 °C
433 °F
[10 K/min], ISO 11357
Eurotec® Tecomid® NB30 MF30 BK001 HS PA6, 30% mineral reinforced, heat stabilized, black
Information provided by Eurotec®
Melting Point 223 °C
433 °F
[10 K/min], ISO 11357
Eurotec® Tecomid® NBX0 GR60 NL PA6, 60% glass fiber reinforced, natural
Information provided by Eurotec®
Melting Point 223 °C
433 °F
10 K/min
BASF Ultradur B 4040 G10 High Speed BK15029 50% Glass Filled PBT/PET
Ultradur B 4040 G10 High Speed BK15029 is a high flow, fast cycling with low warpage, 50% glass filled, injection molding PBT for industrial parts, rigid tough and dimensional stable applications.
Melting Point 223 °C
433 °F
10 K/min
BASF Ultradur B 4300 G2 BK5110 10% Glass Filled PBT
Ultradur B 4300 G2 BK5110 is a pigmented black, easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.
Melting Point 223 °C
433 °F
ISO 11357-1/-2
BASF Ultradur® B 4560 PBT
Description: Medium viscosity injection molding grade for industrial parts in the automotive field, for example for head lamp bezel. Suitable for direct metalizing.Information provided by BASF
Melting Point 223 °C
433 °F
HG/T2235
Beijing Evergrow Resources Oilon
Information provided by Beijing Evergrow Resources.
Melting Point 223 °C
433 °F
10 K/min
BASF Ultradur B 4406 G4 Q113 20% Glass Filled PBT
Ultradur B4406 G4 Q113 is an UL V0 injection molding PBT grade with 20% glass fiber reinforcement.
Melting Point 223 °C
433 °F
ASTM Test
BASF Ultradur B 4406 G6 BKQ113 7110 30% Glass Filled PBT
Ultradur B 4406 G6 BKQ113 7110 is an UL V0 injection molding, pigmented black, PBT grade with 30% glass fiber reinforcement.
Melting Point 223 °C
433 °F
ASTM Test
BASF Ultradur S 4090 G6 LS BK15077 30% Glass Filled PBT
Melting Point 223 °C
433 °F
10 K/min
BASF Ultradur S 4090 G6 LS High Speed BK15077 30% Glass Filled PBT
Ultradur S 4090 G6 LS High Speed BK15077 is a high flow, fast cycling with low warpage, 30% glass filled injection molding PBT.
Melting Point 223 °C
433 °F
10°C/min; DAM; ISO 11357-1/-3
DuPont Performance Polymers Zytel® RS 3261THSL BK041A Nylon 610  (Unverified Data**)
Zytel® RS 3261THSL BK041A is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by weight. It is a black, unreinforced, toughened and heat stabilised r..
Melting Point 223 °C
433 °F
[10 K/min], ISO 11357
Eurotec® Tecomid® NB40 GR30 NL XA60 PA6, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural
Information provided by Eurotec®
Melting Point 223 °C
433 °F
10 K/min; ISO 3146
Eurotec® Tecomid® NB40 MR25 NL IL PA 6 25% mineral reinforced, impact modified
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Melting Point 223 °C
433 °F
[10 K/min], ISO 11357
Eurotec® Tecomid® NB40 NL FN70 PA6, unfilled, flame retardant - halogen free (RoHS compliant), natural
Information provided by Eurotec®
Melting Point 223 - 235 °C
433 - 455 °F
Average value: 231 °C Grade Count:8
Overview of materials for Polymethylpentene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr..
Melting Point 223 °C
433 °F
10 K/min
BASF Ultradur B 4040 G10 LS High Speed BK15029 50% Glass Filled PBT/PET
Melting Point 223 °C
433 °F
DAM; 10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Zytel® RS 3261THSL BK041A Nylon 610  (Unverified Data**)
Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261THSL BK041A is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient..
Melting Point 223 - 227 °C
433 - 441 °F
DSC
Gromax PBT 1200-211M
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Copyright © lookpolymers.com All Rights Reserved