Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 131 °C | 268 °F | Exxon Method |
ExxonMobil Escorene® HD-6705 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Medium Flow, Good Stiffness, Good ImpactUses: Food containers, Housewares, Toys |
|||
Melting Point | 131 °C | 268 °F | ASTM D3417 |
NOVA Chemicals Novapol® HE-D250A HDPE Extrusion Resin
(discontinued **) Features: Excellent ESCR and toughness, good processability.Applications: conduit, corrugated pipe.Data provided by the manufacturer. |
|||
Melting Point | 131 °C | 268 °F | ASTM D3417 |
Total Finathene® 3344N Natural HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
Melting Point | 131 °C | 268 °F | |
LyondellBasell Lupolen® 5021 D HDPE, Blow Molding Grade Easy flow, blow molding grade for small containers (up to 5 l), bottles for surface-active substances, household chemicals, laundry and dishwashing detergents, sanitary cleaners, cosmetics and pharm.. |
|||
Melting Point | 131 °C | 268 °F | |
LyondellBasell Lupolen® 5031 L HDPE, Injection Molding Grade Easy flow, injection molding grade for closures, aerosol pumps, spray nozzles for spray cans, small automotive parts such as the caps on lead/acid batteries, knobs, barrels for writing instruments a.. |
|||
Melting Point | 131 °C | 268 °F | ASTM D2117 |
Global B-8200 High Density Polyethylene Description-high molecular weight, excellent stress cracking resistance,
excellent impact strength to blow moldApplications-large drums, gasoline tanks, agricultural chemical tanksInformation provi.. |
|||
Melting Point | 131 °C | 268 °F | ASTM D2117 |
Global J-1600 High Density Polyethylene Description-suitable for injection moldingApplications-household products, handy craft flowers, toys, stationaryInformation provided by Global Polymers Corporation. |
|||
Melting Point | 131 °C | 268 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ H5814J High Density Polyethylene Injection Molding Key Characteristics:Good processabilityHigh stiffnessHigh impact strengthBalanced properties between shrinkage and warpageOdorlessSafe for food contactRecommended Applications: General purpose inje.. |
|||
Melting Point | 131 °C | 268 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ H5818J High Density Polyethylene Injection Molding Key Characteristics:Good processabilityHigh stiffnessHigh impact strengthBalanced properties between shrinkage and warpageOdorlessSafe for food contactRecommended Applications: General purpose inje.. |
|||
Melting Point | 131 °C | 268 °F | ISO 11357-3 |
Borealis VL4470 High Density Polyethylene VL4470 is a high density polyethylene. Applications: Blown film, Rashel knitted and woven fabrics, and Stretch tape.Information provided by Borealis AG |
|||
Melting Point | 131 °C | 268 °F | ASTM D3417 |
Total HDPE XT25N High Density Polyethylene, Pipe Resin Polyethylene: High molecular weight, bimodal pipe resin. PPI TR4 designation PE4710 /PE100 for demanding installations. Every batch certified to meet 2500 hrs PENT according to ASTM F1473.Charact.. |
|||
Melting Point | 131 °C | 268 °F | ISO 11357 |
Total Lumicene® mPE M5220 Metallocene High Density Polyethylene This product is a Total Ecosolutions grade.Lumicene® mPE M 5220 is a High Density Polyethylene with very good organoleptic properties, dimensional stability, stress-cracking resistance, rigidity an.. |
|||
Melting Point | 131 °C | 268 °F | DSC |
Formosa Plastics Formolene® E925 Film HDPE High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E925 is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristics.. |
|||
Melting Point | 131 °C | 268 °F | DSC; ISO 11357-3 |
Borealis VL5580 High Density Polyethylene VL5580 is a high density polyethylene. This grade is especially designed for monofilament and cast film stretch tape production. Applications: ropes, twines , nets, monofilament applications, stra.. |
|||
Melting Point | 131 °C | 268 °F | ASTM D3417 |
Total HL 428 HDPE Film Grade Medium molecular weight grade. Excellent processability, excellent compatibility with LDPE and LLDPE, good tear and impact strength, good stiffness, excellent drawdown, and good moisture barrier pro.. |
|||
Melting Point | 131 °C | 268 °F | Equate Test Method |
Equate EGDA-6888 HDPE Film Extrusion Resin EGDA-6888 is a high molecular weight, high density polyethylene copolymer that has been designed specifically for tubular film extrusion. Its broad molecular weight distribution and density have bee.. |
|||
Melting Point | 131 °C | 268 °F | Dow Method (DSC) |
Dow DMDA-8907 NT 7 High Density Polyethylene Resin DOW DMDA-8904 NT 7 is produced using UNIPOL™ process technology. It is intended for use in injection molding applications such as pails, industrial parts and other shipping containers. Information.. |
|||
Melting Point | 131 °C | 268 °F | Dow Method (DSC) |
Dow UNIVAL™ DMDA-6220 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6220 NT 7 is a multipurpose polymer designed for high speed production of blow molded containers used to package househol.. |
|||
Melting Point | 131 °C | 268 °F | Dow Method (DSC) |
Dow UNIVAL™ DMDA-6320 NT 7 High Density Polyethylene Resin (HDPE) Low swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6320 NT 7 is a multipurpose polymer designed for the high speed production of blow molded containers used to package household.. |
|||
Melting Point | 131 °C | 268 °F | Dow Method (DSC) |
Dow UNIVAL™ DMDC-6143 NT 7 High Density Polyethylene Resin (HDPE) Excellent parison melt strength / low sag Good extrudability / process-ability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDC-6143 NT 7 is a polymer with broad molecular weight distri.. |
|||
Melting Point | 131 °C | 268 °F | Dow Method (DSC) |
Dow UNIVAL™ DMDC-6145 NT 7 High Density Polyethylene Resin (HDPE) Excellent parison melt strength / low sag Good extrudability / process-ability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDC-6145 NT 7 provides good parison stability, which contribu.. |
|||
Melting Point | 131 °C | 267 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil HD 7960.13 HMW Blown Film Resin Product Description: HD 7960.13 is a high molecular weight HDPE blown film resin. Films made from HD 7960.13 exhibit excellent impact and toughness properties, as well as high stiffness. HD 7960.13 .. |
|||
Melting Point | 131 °C | 268 °F | ASTM D3418 |
ExxonMobil HDP8760.29 Rotational Molding Resin Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal.. |
|||
Melting Point | 131 °C | 268 °F | ASTM D3418 |
E-Polymers EFLEX® M300 HDPE M-series: E-FLEX M series resins are a maleic anhydride grafted (MAH) polymer concentrate designed as synthetic rubber and polyolefin manufactured by E-Polymers. It offers excellent adhesion to nyl.. |
|||
Melting Point | 131 °C | 268 °F | ASTM D3418 |
ExxonMobil HD 8760.29 Rotational Molding Resin Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal.. |
|||
Melting Point | 131 °C | 268 °F | DSC |
Formosa Plastics Formolene® LH5204 Injection Molding HDPE
(discontinued **) CopolymerApplications: Pails, lids and over-capsFormolene LH5204 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Administration as .. |
|||
Melting Point | 131 °C | 268 °F | ASTM D3417 |
Total XT10 N Natural HDPE, pipe Applications: Potable water, industrial and mining, sewer and sewer relining, gas and oil gathering, general pipe relining, pipe coatingInformation provided provided by Total Petrochemicals.Total Pe.. |
|||
Melting Point | 131 °C | 268 °F | DSC |
Formosa Plastics Formolene® E927 Film HDPE High Density Polyethylene High Molecular Weight Bi-Modal Resin For Thin Film Applications Formolene® E927 is a high molecular weight grade of HDPE designed for high drawdown to produce thin films w.. |
|||
Melting Point | 131 °C | 268 °F | DSC |
Formosa Plastics Formolene® E927ND Film HDPE High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E927ND is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristi.. |