Material Notes:
Data Provided by Exxon Chemical Canada.Characteristics: Medium Flow, Good Stiffness, Good ImpactUses: Food containers, Housewares, Toys
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ASTM D4883
Environmental Stress Crack Resistance <= 2.0 hour
<= 2.0 hour
F-50; 10% Igepal Cond. B; ASTM D-1693
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
Exxon Method
Melt Flow 19 g/10 min

@Load 2.16 kg,
Temperature 190 °C
19 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Spiral Flow 47.5 cm
18.7 in
Exxon Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.1 MPa
3500 psi
ASTM D638
Elongation at Yield 19 %
19 %
ASTM D638
Flexural Modulus 0.648 GPa
94.0 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 131 °C
268 °F
Exxon Method
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Processing Properties Metric English Comments
Nozzle Temperature 215 °C
419 °F
Nozzle (Melt)