Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 99.0 µm/m-°C @Temperature 20.0 °C |
55.0 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS Centrex® 814 ASA Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba.. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C @Temperature 20.0 °C |
55.0 µin/in-°F @Temperature 68.0 °F |
|
Eastman Tenite 383A-08 Cellulose Acetate Propionate
(discontinued **) 8% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
55.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP KX06415 Acetal Copolymer LNP LUBRICOMP* KX06415 is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid Powder. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6 IM 40 Z Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6 IM HS L Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6 IM L Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6 IM L N Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6 IM L W Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6 IM L W N Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6 IM X Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedProcessing Method: Injection MoldingInformat.. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PBT E IM SL3 Availability: North AmericaForms: PelletsAdditive: Impact Modifier and Silicone LubricantFeatures: Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® POM CO IM MB Availability: North AmericaForms: PelletsAdditive: Impact Modifier Features: Impact Modified and CopolymerInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® ASA 814 GY Availability: North AmericaForms: PelletsFeatures: Good Weather ResistanceAppearance: GrayInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
55.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON SD000 PA12 LNP* STAT-KON* SD000 is an unfilled Nylon 12 compound. Added feature of this grade is: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® POM CO E TL20 Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated, Good Wear Resistance and CopolymerProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® POM CO TL20 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated, Good Wear Resistance, Low Friction and CopolymerUL File Number: E157318Information provided by TP Composit.. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® POM HO TL20 BN042 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated and HomopolymerAppearance: Brown, Natural Color and RedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PA6/6,6 IM HS L Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedProcessing Method: Injection Mold.. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PA6/ABS 1120 B1 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Information provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PA6/ABS 1120 GF4 4% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 4% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedInformation provided by TP Composites, .. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
55.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP TH0300B PU LNP* Thermocomp* Th0300B is a compound based on Polyurethane containing proprietary fillers. Characteristics of this grade are High Specific Gravity. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
55.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP KAL22M Acetal Copolymer LNP LUBRICOMP* KAL22M is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PA6/ABS 1120 B1 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PA6 IM A Nylon 6 Availability: North AmericaForms: PelletsAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Conductive, Impact Modified, Heat Stabilized and LubricatedAppearance: BlackInformation pro.. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PA6 IM B Nylon 6 Availability: North AmericaForms: PelletsAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Conductive, Impact Modified, Heat Stabilized and LubricatedAppearance: Off-WhiteInformation.. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6 FR-N IM Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Flame Retardant, Heat Stabilized, Impact Modified, Halogen Free and Lubricated Appearance: .. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® POM HO TL20 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated and HomopolymerInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C | 55.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® POM HO TL20 BK Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated and HomopolymerAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C @Temperature 20.0 °C |
55.0 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS Centrex® 825 ASA+AES Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionThermoformi.. |
|||
CTE, linear, Parallel to Flow | 99.0 µm/m-°C @Temperature -30.0 - 100 °C |
55.0 µin/in-°F @Temperature -22.0 - 212 °F |
ISO 11359-2 |
SABIC Innovative Plastics SABIC PPCOMPOUND 5310 PP SABIC® PPcompound 5310 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and heat stability with exterior automotive weathering stability. The IMDS I.. |