Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion L4536 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion L7703 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycolac® MG37EPX ABS ABS plating grade optimized for a broad processing window for both painted and plated applications. NSF standard 61 compliant (80 sq in/L) |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycolac® MG37EPX ABS (Europe-Africa-Middle East) ABS plating grade optimized for a broad processing window for both painted and plated applications. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXL8454 PC COPOLYMER (Asia Pacific) Lexan* EXL8454 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 50% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX2289 PC (Europe-Africa-Middle East) Lexan* LUX2289 resin is an injection molding grade with high light reflectance and UV stabilized |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
33.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX7189 PC Lexan* LUX7189 is an injection moldable, high light reflectance FR grade. Contains non-brominated, non-chlorinated flame retardant systems. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 315 Z H2.0 901510 Nylon 6, 15% Glass Fiber PA 6 extrusion- and blow molding-grade with 15% glass fibers, branched/structural viscosity, elastomer-modified, good heat-ageing resistance, dry-impact modifiedApplication Examples: air intake hose.. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
33.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Stat-kon DD0009XQ PC (Europe-Africa-Middle East) LNP* Stat-Kon* DD0009XQ is a compound based on Polycarbonate containing Carbon Powder and Flame Retardant. Added features include Electrically Conductive, Flame Retardant and Easy Molding.This data.. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® VX5005 PBT (Europe-Africa-Middle East) VALOX VX5005 is a 5% glass fibre reinforced, impact modified PBT+PC blend with low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
33.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP AX04518 ABS LNP* THERMOCOMP* AX04518 is a compound based on ABS resin containing proprietary filler(s). |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl HB1525 PPE+HIPS (Europe-Africa-Middle East) NORYL HB1525 is a 15 % short glass fibre reinforced material with a HDT/A of 115°C according ISO 75. NORYL HB1525 is an easy flow material designed for applications where dimensional stability an.. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL PX5511E PPE+HIPS (Europe-Africa-Middle East) Noryl PX5511E is an unfilled material with good flow and chemical resistance against cleaners. Noryl PX5511E is developed for personal care appplications. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
33.3 µin/in-°F @Temperature -22.0 - 176 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 9085 PEI Blend (Europe-Africa-Middle East) High flow Polyetherimide blend. Meets FAR 25.853 and OSU 55/55 with low toxicity, smoke and flame evolution. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ISO 11359 |
Styrolution Terblend® N NG-02 8% Glass Filled ABS/PA6 (Dry) Terblend N NG-02 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, high impact strength and good surface appearance.Information provided by STYROLUTION, which is a join.. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 20.0 °C |
33.3 µin/in-°F @Temperature 68.0 °F |
|
Covestro Makrolon® 3158 Polycarbonate Key Features:Release agentUnfilledSuitable processing methods:Injection moldingExtrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated.. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TSS/2 FA PA666 Product description: Grilon TSS/2 FA is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS/2 FA has the following important properties: Excellent flow .. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
33.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AK8 PA66, 40% Mineral Reinforced, Injection Molding Staramide AK8 is a 40% Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
33.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AK8ST41 PA66, Mineral Reinforced, Impact Modified, Injection Molding Staramide AK8ST41 is an Impact Modified, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 20.0 °C |
33.3 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Dow Tyril® 990 SAN TYRIL® 990 SAN copolymer grade provides colorless glass-like clarity and excellent overall optical properties. It provides a profile of very good strength with stiffness, chemical resistance, heat .. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ISO 11359-1/-2 |
Covestro Makroblend® DP 2-7655 MBS162 Polycarbonate + PET, Mineral Filled Impact Grade Developmental product(PC+PET)-blendsimpact modifiedInjection molding grade 10% mineral filledAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new .. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
33.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam AFR662B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR662B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 20.0 °C |
33.3 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® AZM 23 G9 T6LD Nylon 12, 23% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-050,(G+C)(F+D)(23+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C @Temperature 20.0 °C |
33.3 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® AZM 23 T6LD Nylon 12, 23% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-050,GF23Rigid grade with glass fiber filler (23%) for injection molding. Available colors: black and natural. Reinforced light and heat stabilizing agent. Mold-rele.. |
|||
CTE, linear, Parallel to Flow | 60.0 - 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 44.4 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® KR 4350 BK 00464 PA6/6T (Dry) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
CTE, linear, Parallel to Flow | 60.0 - 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 44.4 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® KR 4350 PA6/6T (Dry) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
CTE, linear, Parallel to Flow | 60.0 - 100 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 55.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® C3U PA66/6 (Dry) Ultramid C3U is an injection molding, general purpose PA66/6 grade with improved flame retardance. |
|||
CTE, linear, Parallel to Flow | 60.0 µm/m-°C | 33.3 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® DP 7102 000000 PBT, 30% Mineral
(discontinued **) PBT, 30% mineral, injection molding, LDS |