Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 45.0 µm/m-°C | 25.0 µin/in-°F | ASTM D696 |
PolyOne Nanoblend™ LST 5501 Polypropylene, Unspecified (PP, Unspecified) Nanoblend compounds, formerly known as Maxxam LST, are LIGHT, STIFF AND TOUGH. Using nanoclay technology, these compounds deliver a combination of high stiffness and impact resistance to meet demand.. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
25.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP FARADEX DX92079 PC (Europe-Africa-Middle East) LNP* Faradex* DX92079 is a compound based on Polycarbonate resin containing Glass Fiber, Glass Bead, Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding, Mold Release... |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
25.0 µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula.. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C | 25.0 µin/in-°F | ASTM D696 |
LG Chemical LUMID GP2200A(W) PA6+GF20%, General Purpose Feature: Injection Molding, PA6+MF23%, High ImpactPA6+GF20%, General PurposeApplication: HMID, SLMP B, HolderCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C @Temperature 20.0 °C |
25.0 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
Mitsubishi Xantar® G2F 23 R Polycarbonate-10% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C @Temperature 20.0 °C |
25.0 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
Mitsubishi Xantar® G2F 23 UR Polycarbonate-10% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRILOY UA200A PPA LNP LUBRILOY* UA200A is a compound based on Polyphthalamide resin containing Aramid Fiber, Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRILOY UA200A PPA (Asia Pacific) LNP LUBRILOY* UA200A is a compound based on Polyphthalamide resin containing Aramid Fiber, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
25.0 µin/in-°F @Temperature -58.0 - 122 °F |
1 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK) AvaSpire® AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been for.. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C | 25.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP GF15 CC 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C | 25.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP GF20 CC HS 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and Chemically CoupledInformation pro.. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C | 25.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PVDF CF15 BK 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 15% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C | 25.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PVDF CF15-M BK 15% Milled Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Carbon Fiber, 15% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
25.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP DFB03GR PC (Europe-Africa-Middle East) LNP* THERMOCOMP* DFB03GR is a compound based on Polycarbonate resin containing a mixture of Glass Fiber and Glass Beads. Added features of this material include: Easy Molding. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C | 25.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PBT GF10 CBA 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: FoamableAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C | 25.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PP GF20 CC 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C | 25.0 µin/in-°F | ASTM D696 |
Styron VELVEXâ„¢ 5250 SC Reinforced Elastomer/PP compound Overview: VELVEXâ„¢ 5250 SC Natural is a reinforced elastomer/PP compound which provides a unique property balance of good stiffness, impact and high heat resistance in combination with a nice so.. |
|||
CTE, linear, Parallel to Flow | 45.0 - 55.0 µm/m-°C @Temperature 20.0 °C |
25.0 - 30.6 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit 4451 XB Novolac Phenolic Organic and mineral filled phenolic molding compound with excellent mechanical properties (highest notched impact strength).USES: Fuse holders, brush holders, circuit breakers, automotive ignition a.. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
25.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam BFR552Y3 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR552Y3 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
25.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam BFR552Y6 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR552Y6 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
25.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starglas FF004 HDPE, Glass Fiber Filled Starglas FF004 is a Glass Fiber Reinforced High Density Polyethylene ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
25.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide ALY540A PA66, Glass/Mineral Fiber Reinforced, Injection Molding Staramide ALY540A is a Glass Fiber Reinforced, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C @Temperature 20.0 °C |
25.0 µin/in-°F @Temperature 68.0 °F |
|
BASF Luranyl® KR 2454/3 G2 Polyphenylene Ether + Styrene-Butadiene Blend, 10% Glass Fiber Reinforced Heat resistant grade with halogen-free flame retardant; applications include TV plug connectors and components in switchgear cabinets.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
25.0 µin/in-°F @Temperature 73.4 - 131 °F |
DIN 53752 |
BASF Ultraform® N2720 M63 30% Mineral Filled POM Description: Is a POM, 30 % mineral-reinforced material for low-warpage moldings with high stiffness, strength and hardness.Information provided by BASF |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
25.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOTUF WF003I PBT (Europe-Africa-Middle East) LNP* Thermotuf* WF003I BLACK is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C | 25.0 µin/in-°F | Below Tg, Result based on HT G22; ISO 11359 |
Victrex® HT™ G45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia.. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C | 25.0 µin/in-°F | Below Tg; ISO 11359 |
Victrex® PEEK 650G Polyetheretherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C | 25.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® TPU GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 45.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
25.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp FF004 PE (Europe-Africa-Middle East) LNP* THERMOCOMP* FF004 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |