Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Halar® 513LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Information provided by Solvay Specialty Polymers. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Halar® 902 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)< Information provided by Solvay Specialty Polymers. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® CI 31 F 000000 Copolyamide PA6/6I Copolyamide PA6/6I, low melt point (188-191°C), low viscosity, no additives, very high transparency, in compliance with FDA as far as the PA-layer is separated from the food by a 50 µm PE film.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® S 1506 000000 PBT PBT, non-reinforced, injection molding extrusion, impact modified |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | |
Solvay Specialty Polymers Ajedium™ Films -- Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Halar® ECTFE is a semi-crystalline fluoropolymer with a chemical structure of a 1:1 alternating copolymer of ethylene and chlorotrifluoroethylene.Halar® film is a strong, hard, tough, abrasion.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | |
Solvay Specialty Polymers Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation prov.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | |
Solvay Specialty Polymers Halar® 930LCW Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 23.0 - 80.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
Styrolution Terblend® N NM-19 XP Beige 38163 ABS+PA (Dry) Description: Terblend® N NM-19 XP is an UV stabilized ABS/PA blend combining very high impact strength, even at low temperatures with an outstanding processability and excellent surface appearanc.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
|
Eastman Eastar GN007 PETG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K240-HP (Dry) Impact Modified Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® E53 NC010 Nylon 66 Unreinforced High Viscosity Polyamide 66 Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® S223-DK Nylon 66 (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature -40.0 - 23.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
|
BASF Polystyrol® 476 L Impact Grade Polystyrene (Europe) Normal flowing, high-impact grade. When extruded it is often mixed with PS 165 H.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
|
BASF Polystyrol® 2712 Impact Grade Polystyrene (Europe) Easy flowing special grade, particularly resistant to stress cracking.Data was collected by ISO methods and provided by BASF. |