Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -8.00 °C | 17.6 °F | TR test, TR70 |
Daikin DAI-EL G-501NK Fluoroelastomer Terpolymer, Diamine Curable Grade, 68% Fluorine Content Features: Good mechanical characteristics.Information provided by Daikin Industries. |
|||
Minimum Service Temperature, Air | -8.00 °C | 17.6 °F | TR test, TR70 |
Daikin DAI-EL G-558 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 69% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Low gasoline permeability and good.. |
|||
Minimum Service Temperature, Air | -8.00 °C | 17.6 °F | TR test, TR10 |
Daikin DAI-EL G-603 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 71% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Information provided by Daikin Industries. |
|||
Minimum Service Temperature, Air | -8.00 °C | 17.6 °F | TR test, TR10 |
Daikin DAI-EL G-621 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 71% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: General purpose with excellent sol.. |
|||
Minimum Service Temperature, Air | -8.00 °C | 17.6 °F | TR test, TR70 |
Daikin DAI-EL G-702 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: General purpose with excellent elongation and tear strength.Informatio.. |
|||
Minimum Service Temperature, Air | -8.00 °C | 17.6 °F | Gehman torsion test, T2 |
Daikin DAI-EL G-702 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: General purpose with excellent elongation and tear strength.Informatio.. |
|||
Minimum Service Temperature, Air | -8.00 °C | 17.6 °F | Gehman torsion test, T2 |
Daikin DAI-EL G-704 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |
|||
Minimum Service Temperature, Air | -8.00 °C | 17.6 °F | TR test, TR70 |
Daikin DAI-EL G-704 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |
|||
Minimum Service Temperature, Air | -8.00 °C | 17.6 °F | TR test, TR70 |
Daikin DAI-EL G-755 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Extrusion of hose and tubing, etc.Information provided by Daikin Indus.. |
|||
Minimum Service Temperature, Air | -8.00 °C | 17.6 °F | TR test, TR70 |
Daikin DAI-EL G-763 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Excellent mold releasability for O-rings.Information provided by Daiki.. |
|||
Minimum Service Temperature, Air | -8.00 °C | 17.6 °F | Gehman torsion test, T2 |
Daikin DAI-EL G-783 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Fast vulcanization, for complex shapes.Information provided by Daikin .. |
|||
Minimum Service Temperature, Air | -8.00 °C | 17.6 °F | TR test, TR10 |
Daikin DAI-EL G-901 Fluoroelastomer Terpolymer, Peroxide Curable Grade, 71% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Excellent solvent resistance.Information provided by Daikin Industries. |
|||
Minimum Service Temperature, Air | -8.00 °C | 17.6 °F | TR test, TR10 |
Daikin DAI-EL G-902 Fluoroelastomer Terpolymer, Peroxide Curable Grade, 71% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Excellent solvent resistance, good mold flow.Information provided by Daikin Industries. |
|||
Minimum Service Temperature, Air | -8.00 °C | 17.6 °F | TR test, TR70 |
Daikin DAI-EL G-952 Fluoroelastomer Terpolymer, Peroxide Curable Grade, 69% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Good solvent resistance and low-temperature characteristics.Information provided by Daikin Industrie.. |
|||
Minimum Service Temperature, Air | -8.00 °C | 17.6 °F | TR test, TR70 |
Daikin DAI-EL G-551 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 69% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Products with excellent balance of.. |
|||
Minimum Service Temperature, Air | -8.00 °C | 17.6 °F | TR test, TR10 |
Daikin DAI-EL G-912 Fluoroelastomer Terpolymer, Peroxide Curable Grade, 71% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Excellent solvent resistance, good compression set.Information provided by Daikin Industries. |