Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® 2285-2 Extruded PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® 280-6(R) Roll Covering Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® G565 Glass Cloth Backing Silicone Adhesive Pressure Sensitive Tape Description: Glass cloth offers excellent abrasion resistance and mechanical properties, as well as high tensile strength and extreme temperature resistance. Service temperatures range from -100°.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® M741 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® M815 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® SG05-14(R) Premium Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® SG06-05(R) Premium Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® SG26-05(R) Primary Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® SG36-05(R) Industrial Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® SGB6-06(R) CHEMLAM Brown Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® 2042-2 Skived PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® A-2005 Industrial Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® C663 Paper Backing Silicone Adhesive Pressure Sensitive Tape Description: Paper tapes are designed to provide high temperature and excellent solvent resistance for wave soldering, printed circuit board masking, and hot air leveling applications. Service tempe.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® K100 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® K250 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Saint-Gobain CHR® M52 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Master Bond EP21TDCF-3 Two Component, Higher Viscosity Epoxy System Product Description: Master Bond EP21TDCF-3 is a two component epoxy for high performance bonding and sealing. It is formulated to cure rapidly at room temperature or faster at elevated temperatures.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Master Bond Supreme 11AN Two Component, Heat Resistant Epoxy Adhesive Description: Master Bond Polymer Adhesive System Supreme 11AN is a two component thermally conductive heat resistant epoxy adhesive with a one-to-one mix ratio, by weight or volume. It readily devel.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Master Bond Supreme 11HT High Temperature Resistant Two Component Epoxy System Master Bond Polymer System Supreme 11HT is an easy to use two part epoxy adhesive/sealant combining both high shear and high peel strengths along with a relatively fast cure at room temperature. Sup.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Arlon CP-RC-3916 Bulk Compound This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Arlon R30370A008 0.008" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 0.001" FEP FilmSide 1: Unsupported/Uncured Silicone RubberSubstrate: 0.003" PTFE coated FiberglassThis data represents typical values for the production material a.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Arlon R36580N008 0.008" ((0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassAppearance: Grey silicone gumThis data represents typical values for the production material. The dat.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Arlon Thermabond® 48A51X015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Primerless Thermabond® Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubb.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Arlon Thermabond® 99950N008 Silicone Rubber/Fiberglass Laminate Electrically conductive, Thermabond®. primerless. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Arlon Thermabond® 99950N015 Silicone Rubber/Fiberglass Laminate Electrically conductive, Thermabond®. primerless. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Arlon Thermabond® R36200A008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated Fiberglass Appearance: Blue silicone gumThis data represents typical values for the production material. The d.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Arlon R3781-920-##R##-P0 Silicone Rubber This fusible silicone tape is specially formulated to yield improved flexibility, elongation and elastic recovery at low operating temperature (-70°C to -100°C) where standard fusible silicone tap.. |
|||
Minimum Service Temperature, Air | -73.3 °C | -100 °F | |
Master Bond Supreme 46HT-2ND2 Two Component, Non-Drip, Toughened, Epoxy Adhesive Master Bond Polymer Supreme 46HT-2ND2 is a two component, non-drip, epoxy adhesive featuring an attractive balance of superior shear and peel strengths for high performance structural bonding suitab.. |