Polymer Property : Minimum Service Temperature, Air = -240 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -240 °C
-400 °F
Manifattura Cattaneo PTFE Polytetrafluoroethylene
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Minimum Service Temperature, Air -240 °C
-400 °F
Manifattura Cattaneo RULON® W2 Polytetrafluoroethylene
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Minimum Service Temperature, Air -240 °C
-400 °F
Garlock GRAPH-LOCK® 3124/3126 Graphite Sheet Gasketing, Steel Wire Insert
A laminated graphite sheet with a 316SS wire mesh insert.Pure exfoliated graphite flake material excels in extreme conditions, withstanding heat, pressure, and aggressive chemicalsProven fire-safeSe..
Minimum Service Temperature, Air -240 °C
-400 °F
Garlock GRAPH-LOCK® 3125SS Graphite Sheet Gasketing, Steel Foil Insert
A laminated graphite sheet with a 316SS foil insert.Pure exfoliated graphite flake material excels in extreme conditions, withstanding heat, pressure, and aggressive chemicalsProven fire-safeSeals e..
Minimum Service Temperature, Air -240 °C
-400 °F
Garlock GRAPH-LOCK® 3128 HOCHDRUCK® Graphite Sheet Gasketing, Steel Reinforced
High performance multi-layer graphite with 316SS inserts provides high compressive strength, blow-out resistance, excellent handling properties and improved tightness.Pure exfoliated graphite flake ..
Minimum Service Temperature, Air -240 °C
-400 °F
GrafTech GRAFOIL® GHC Standard Internal Combustion Laminate
GRAFOIL® Grade GHC is a laminate made from Grade GTC flexible graphite. Laminate Construction: GRAFOIL® Grade GTC ? Micro-thin, phenolic-based adhesive ? GRAFOIL® Grade GTC
Minimum Service Temperature, Air -240 °C
-400 °F
GrafTech GRAFOIL® GHE Standard Fluid Sealing Laminate, Metal Reinforced
GRAFOIL® Grade GHE laminate is made with GTB flexible graphite mechanically bonded to both faces of a 316 or 316L stainless steel tang metal insert. Surface identifiable, the laminate is branded ..
Minimum Service Temperature, Air -240 °C
-400 °F
GrafTech GRAFOIL® GHN Standard Fluid Sealing Laminate, Non-Metal Reinforced
GRAFOIL® Grade GHN is an unbranded laminate made with GRAFOIL® Grade TG-337 flexible graphite, thermally bonded to both faces of a plastic insert. It is not certified to any industry standards..
Minimum Service Temperature, Air -240 °C
-400 °F
GrafTech GRAFOIL® GHR Standard Fluid Sealing Laminate, Metal Reinforced
GRAFOIL® Grade GHR is an uncured laminate made with GRAFOIL® Grade GTB flexible graphite adhesively bonded to both faces of a 0.002" thick flat 316 or 316L stainless steel insert. Surface iden..
Minimum Service Temperature, Air -240 °C
-400 °F
GrafTech GRAFOIL® GTB Standard Fluid Sealing Graphite Single Layer Gasketing Material
GRAFOIL® GTB flexible graphite sheet is a gasketing material containing no binders or fillers. Standard industrial grade GTB flexible graphite has an oxidation/corrosion inhibitor and is typicall..
Minimum Service Temperature, Air -240 °C
-400 °F
GrafTech GRAFOIL® GTC Standard Internal Combustion Graphite, Single Layer Material
GRAFOIL® GTC flexible graphite sheet is a gasketing material containing no binders or fillers, which will seal a wide variety of liquids and gases over an extremely large temperature range. GTC c..
Minimum Service Temperature, Air -240 °C
-400 °F
GrafTech GRAFOIL® GTJ Standard Fluid Sealing Graphite, Single Layer Material
GRAFOIL® GTJ premium flexible graphite is an oxidation/corrosion inhibited grade developed for use in nuclear and high temp, high purity applications. It is certified to meet the most rigorous pu..
Minimum Service Temperature, Air -240 °C
-400 °F
GrafTech GRAFOIL® SUPER GTO® Standard Internal Combustion Single Layer Gasketing Material
GRAFOIL® SUPER GTO® flexible graphite sheet is a gasketing material containing no binders, which will seal a wide variety of liquids and gases over an extremely large temperature range (-240Â..
Minimum Service Temperature, Air -240 °C
-400 °F
Saint-Gobain Norton® Fluorglas® Chemfilm® DF1400 Non-Conductive PTFE Tape
Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super..
Minimum Service Temperature, Air -240 °C
-400 °F
Embrittlement Temp
Saint-Gobain Rulon® 125 Bearing/Seal PTFE
Rulon 125 is used primarily in applications that are not severe such as dryer drum slides and piston rings in pneumatic or hydraulic controls.Information provided by distributor TriStar Plastics Cor..
Minimum Service Temperature, Air -240 °C
-400 °F
Saint-Gobain Rulon® 1410 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
Minimum Service Temperature, Air -240 °C
-400 °F
Saint-Gobain Rulon® 1439 Bearing/Seal PTFE
Rulon® 1439 is a white FDA compliant material that is suitable for immersed service with better wear characteristics than most other PTFE compounds. Its color makes it aesthetically pleasing for ..
Minimum Service Temperature, Air -240 °C
-400 °F
Saint-Gobain Rulon® 488 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
Minimum Service Temperature, Air -240 °C
-400 °F
Saint-Gobain Rulon® 641 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
Minimum Service Temperature, Air -240 °C
-400 °F
Saint-Gobain Rulon® 945 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
Minimum Service Temperature, Air -240 °C
-400 °F
Embrittlement Temp
Saint-Gobain Rulon® 954 Bearing/Seal PTFE
A conductive PTFE material that is available in tape, sheet (extruded) and rod (extruded).Information provided by distributor TriStar Plastics Corp.
Minimum Service Temperature, Air -240 °C
-400 °F
Saint-Gobain Rulon® 957 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
Minimum Service Temperature, Air -240 °C
-400 °F
Embrittlement Temp
Saint-Gobain Rulon® DC7035 Bearing/Seal PTFE
Offers electrical conductivity in a low wear, self lubricating bearing material. This material is ideal in applications where static dissipation is needed. DC7035 is often used as a static bleed mec..
Minimum Service Temperature, Air -240 °C
-400 °F
Saint-Gobain Rulon® LR Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
Minimum Service Temperature, Air -240 °C
-400 °F
Saint-Gobain Rulon® XL Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
Minimum Service Temperature, Air -240 °C
-400 °F
Saint-Gobain Norton® Fluorglas® Chemfilm® DF2919 Fluoropolymer Tape
Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super..
Minimum Service Temperature, Air -240 °C
-400 °F
XADC-Armoloy Diamond-Chrome Composite Coating
XADC-Armoloy® combines the Armoloy® TDC chromium coating with spherical diamond particulates. The XADC-Armoloy® coating enhances the durability of components used in a wide range of applications..
Minimum Service Temperature, Air -240 °C
-400 °F
Embrittlement Temp
TriStar Ultracomp UC-400 Composite Bearing
Ultracomp UC-400 - Designed for high loads, low speeds, impact and vibration applications. UC-400 has a MOS2 additive for salt water applications where cathodic reactions could occur. Excellent dry ..
Minimum Service Temperature, Air -240 °C
-400 °F
Chesterton 800 GoldEnd® Tape
Chesterton® 800 GoldEnd® Tape is a high density moldable, dry PTFE thread sealing tape. It is a heavy duty, tear-resistant product containing more PTFE per inch than virtually any thread sealing t..
Minimum Service Temperature, Air -240 °C
-400 °F
Chesterton 850 Premium Sealing Tape
Description: Chesterton® 850 Premium Sealing Tape is a high density, moldable, dry PTFE thread sealing tape. It is a heavy duty, tear-resistant product containing more PTFE per inch than virtually ..