Material Notes:
A laminated graphite sheet with a 316SS wire mesh insert.Pure exfoliated graphite flake material excels in extreme conditions, withstanding heat, pressure, and aggressive chemicalsProven fire-safeSeals easily under moderate bolt load, offers superior torque retentionRetains dimensional stability in high temperatures; seals tightly even during pressure fluctuationsInformation provided by Garlock Rubber Technologies
Physical Properties Metric English Comments
Permeability 0.10
0.10
Gas Permeability, cc/min; DIN 3535 Part 4
Mechanical Properties Metric English Comments
Tensile Strength 22.8 MPa
3300 psi
ASTM F152
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 649 °C
1200 °F
Steam
454 °C

@Pressure 13.8 MPa
850 °F

@Pressure 2000 psi
Minimum Service Temperature, Air -240 °C
-400 °F
Component Elements Properties Metric English Comments
Carbon, C 98 %
98 %
Industrial Grade
99.5 %
99.5 %
Nuclear Grade
Descriptive Properties Value Comments
Compressibility, % 40
ASTM F36
Creep Relaxation, % 17
ASTM F38
Sealability ASTM F37B, ml/hr 0.2
Nitrogen
1.5
ASTM Fuel A