Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 245 °C | 473 °F | STN EN ISO 306 |
Plastcom SLOVAMID® 6 NG1 GF 30 HLS PA6 reinforced with glass fiber, UV stabilized, hydrolysis resistant PA 6 for injection molding, reinforced with 30% glass fiber, for moldings used in the automotive, weather and UV stabilized. Determined for using in outside automotive applications like door handle,.. |
|||
Vicat Softening Point | 245 °C | 473 °F | 9.8 N; ASTM D1525 |
Nilit Polynil® C50L Externally Lubricated PA66/6 Description: Polynil C50L shows better surface finish, flow and elongation than a comparable homopolymer. Key characteristics: Excellent flowHigh elongationGood impact strengthGood overall mechanica.. |
|||
Vicat Softening Point | 245 °C @Load 5.10 kg |
473 °F @Load 11.2 lb |
50°C/h |
Radici Radilon® A RV250 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Vicat Softening Point | 245 °C | 473 °F | 49 N; ISO 306, ASTM D1525 |
Nilit Nilamid A3 N H2 Nucleated, Heat Stabilized Nylon 66 Description: Nilamid A3 N H2 is a nucleated, heat stabilized NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass production a.. |
|||
Vicat Softening Point | 245 °C @Load 5.00 kg |
473 °F @Load 11.0 lb |
|
LATI Latamid 66 H2 G/50-V0HF1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Eu.. |
|||
Vicat Softening Point | 245 °C @Load 5.00 kg |
473 °F @Load 11.0 lb |
|
LATI Latamid 66 E21 G/30 PA 66, 30% Glass Fiber Reinforced Polyamide 66 (PA66) based compound. Toughened. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici.. |
|||
Vicat Softening Point | 245 °C @Load 5.00 kg |
473 °F @Load 11.0 lb |
|
LATI Latamid 66 H2 G/25-V0HF1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good mechanical properties. Very good electrica.. |
|||
Vicat Softening Point | 245 °C @Load 5.00 kg |
473 °F @Load 11.0 lb |
|
LATI Latamid 66 H2 G/25-V0KB1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Vicat Softening Point | 245 °C @Load 5.00 kg |
473 °F @Load 11.0 lb |
|
LATI Latilub 66-10T Y/15 PA66, 15% Aramid Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). PTFE. Aramid fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri.. |
|||
Vicat Softening Point | 245 °C @Load 5.00 kg |
473 °F @Load 11.0 lb |
|
LATI Latishield 66-08A G/25-V0KB1 PA66, Steel/Glass Fiber Reinforced, Flame Retardant EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Vicat Softening Point | 245 °C @Load 5.00 kg |
473 °F @Load 11.0 lb |
|
LATI Latistat 66-06 PA66 Dissipative product based on Polyamide 66 (PA66). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici.. |
|||
Vicat Softening Point | 245 °C | 473 °F | B/120; ISO 306 |
Sax Polymers SAXAMID 226 Nylon 6.6 SAXAMID 226 is a general purpose polyamide 6.6 injection-molding-grade. Benefits are short cycle times and good release properties.Information provided by SAX Polymers |
|||
Vicat Softening Point | 245 °C | 473 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL GTX GTX909 PPE+PS+PA (Asia Pacific) 400F (205C) HDT. 3.3 Notched Izod. Excellent chemical resistance |
|||
Vicat Softening Point | 245 °C | 473 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Vicat Softening Point | 245 °C | 473 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Europe-Africa-Middle East) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Vicat Softening Point | 245 °C | 473 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX918WR PPE+PA (Asia Pacific) High flow PPE+PA for under-the-hood and electrical applications. With mold release |
|||
Vicat Softening Point | 245 °C | 473 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Noryl GTX GTX918WR PPE+PS+PA (Asia Pacific) High flow PPE+PS+PA for under-the-hood and electrical applications. With mold releaseThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 245 °C | 473 °F | ISO 306 |
Tisan TISLAMID® 66 30% Glass Bead Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Vicat Softening Point | 245 °C | 473 °F | ISO 306 |
Tisan TISLAMID® 66 30% Glass Filled Impact Modified, Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Vicat Softening Point | 245 °C | 473 °F | |
Covestro Baydur® GS PIR B Polyurethane PIR casting system for the production of solid components. Mechanical properties can be varied by adjusting the mixing ratio in the range 1:1-1:2.Information provided by Bayer.As of 1 September 2015.. |
|||
Vicat Softening Point | 245 °C | 473 °F | B/120; ISO 306 |
Eurostar Staramide ALY430A PA66, Glass Fiber Reinforced, Injection Molding Staramide ALY430A is a Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 245 °C | 473 °F | B/50; ISO 306 |
Eurostar Starflam AFR450X2 PA66, 25% Glass Filled, Injection Molded AFR450X2 is a Red Phosphorous, Flame Retardant, 25% Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive su.. |
|||
Vicat Softening Point | 245 °C | 473 °F | B/120; ISO 306 |
Eurostar Starflam AFR470X2 PA66, 35% Glass Filled, Injection Molded AFR470X2 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Vicat Softening Point | 245 °C @Load 5.10 kg |
473 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NA40 GB30 NL HS PA6.6, 30% glass bead reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Vicat Softening Point | 245 °C @Load 5.10 kg |
473 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NA40 MF40 BK001 HS PA6.6, 40% mineral filled, heat stabilized, black Information provided by Eurotec® |
|||
Vicat Softening Point | 245 °C | 473 °F | 50N; ISO 306 |
Eurotec® Tecomid® NA40 NL FA 50 PA 6.6 unreinforced, UL94 V0, halogen/phosphorus free Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Vicat Softening Point | 245 °C @Load 5.10 kg |
473 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NA40 NL FA50 PA6.6, unfilled, flame retardant - halogen free, natural Information provided by Eurotec® |
|||
Vicat Softening Point | 245 °C @Load 5.10 kg |
473 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NA40 NL XA70 PA6.6, unfilled, flame retardant - halogen free (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Vicat Softening Point | 245 °C @Load 5.10 kg |
473 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NT40 NL PPA, unfilled, natural Information provided by Eurotec® |
|||
Vicat Softening Point | 245 °C @Load 5.10 kg |
473 °F @Load 11.2 lb |
50°C/h |
Radici Radilon® A RV350 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |