Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Vicat Softening Point = 243 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 117 °C

@Load 1.00 kg
243 °F

@Load 2.20 lb
ISO 306/A
Polimeri Europa Clearflex® FH 50 Linear Medium Density Polyethylene
Clearflex FH 50 is a linear medium density polyethylene, with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FH 50 are characterized by a good balance between toug..
Vicat Softening Point 117 °C

@Load 1.00 kg
243 °F

@Load 2.20 lb
ISO 306/A
Polimeri Europa Flexirene® FH 56 A Butene Copolymer Linear Low Density Polyethylene
Flexirene FH 56 A is a butene copolymer with medium density (C4-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Flexirene FH 56 A are characte..
Vicat Softening Point 117 °C
243 °F
Dow Isoplast® 151 Polyurethane (PUR-RT), Impact Modified  (discontinued **)
ISOPLAST® 151 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include excellent chemical resistance, high heat, low mois..
Vicat Softening Point 117 °C
243 °F
ASTM D1525
Chevron Phillips HiD® 9035 HDPE Injection Molding Resin  (discontinued **)
Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 231, A 52600Characteristics: Excellent Flow, Moderate Impact Strength, Good Stiffness, Moderate ESCR, Excellent Shrinkage ResistanceAppli..
Vicat Softening Point 117 °C
243 °F
ASTM D1525
Eastman M2004-P Polyethylene  (discontinued **)
M2004-P polyethylene is suggested for applications such as spiral-wound can linings, release paper and photographic paper. M2004-P has been found to exhibit good barrier properties, temperature res..
Vicat Softening Point 117 °C
243 °F
resin; ASTM D1525
Lotte Chemical Titan TITANEX® MR4086 Medium density polyethylene resin  (discontinued **)
MR4086 is a UV stabilized, pelleted medium density polyethylene for rotomolding.Applications: Large industrial tanks, agriculture tanks, chemical drums, bins, cones, bottle caps.Advantages: Excelle..
Vicat Softening Point 117 °C

@Load 1.02 kg
243 °F

@Load 2.25 lb
Kaneka PHBH Rigid Bio-based Polymer
A copolymer produced of 3-hydroxybutyrate and 3-hydroxyhexanoate produced by fermentation of plant oils. It has excellent biodegradability (under anaerobic, aerobic, aquatic, and compost conditions..
Vicat Softening Point 117 °C
243 °F
ISO 306A
Lucite International Diakon® CMG314V Acrylic Polymer
Information provided by Lucite International
Vicat Softening Point 117 °C
243 °F
ISO 306A
Lucite International Diakon® CMH454L Acrylic Polymer
Information provided by Lucite International
Vicat Softening Point 117 °C
243 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC
Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
Vicat Softening Point 117 °C
243 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Europe-Africa-Middle East)
Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
Vicat Softening Point 117 °C
243 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC
Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty..
Vicat Softening Point 117 °C
243 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Asia Pacific)
Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty..
Vicat Softening Point 117 °C
243 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Europe-Africa-Middle East)
Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty..
Vicat Softening Point 117 °C
243 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Europe-Africa-Middle East)
Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty..
Vicat Softening Point 117 °C
243 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC
Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im..
Vicat Softening Point 117 °C
243 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Europe-Africa-Middle East)
Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp..
Vicat Softening Point 117 °C
243 °F
B/50; ISO R306
Samsung Cheil Industries Infino® HA-1011 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Vicat Softening Point 117 °C
243 °F
B/50; ISO R306
Samsung Cheil Industries Infino® HA-1011 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Vicat Softening Point 117 °C
243 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Valox® V3903WX PBT+PC (Asia Pacific)
Unreinforced fllame retardant PBT/PC blends with good chemical resistance and low temperature impact, UV stablized
Vicat Softening Point 117 °C
243 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC (Asia Pacific)
Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp..
Vicat Softening Point 117 °C
243 °F
Styron Magnumâ„¢ 358HP ABS, High Heat
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Vicat Softening Point 117 °C
243 °F
10 N; ISO 306A
Borealis Borseal™ TD120BF Terpolymer for BOPP Film
Borseal TD120BF is a C2/C4 terapolymer film resin especially developed for use as sealing layers in coextruded BOPP film (manufactured on stenter frame and double bubble film process).Borseal TD120B..
Vicat Softening Point 117 °C
243 °F
ISO 306
Tisan TISOPLEN® 10% Talc Filled Heat Stabilized Homopolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Vicat Softening Point 117 °C
243 °F
A50; ISO 306
Lubrizol ESTANE® GP95AB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 95AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in ..
Vicat Softening Point 117 °C
243 °F
temperature B; ISO 36
Lubrizol ESTALOC® T514 Ester-Type, Reinforced Engineering Thermoplastic (European Grade)
Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio..
Vicat Softening Point 117 °C
243 °F
120°C/hr, 9.8N; ASTM D1525
Lubrizol Estane® 2102-90A Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20..
Vicat Softening Point 117 °C
243 °F
BASF Luranyl® KR 2401 Polyphenylene Ether + Styrene-Butadiene Blend, Impact Grade
Base grade with a balanced combination of impact strength and stiffness. Uses include: parts of vehicle interiors, air ducts and loudspeaker housings.Data was collected by ISO methods and provided ..