Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 100 °C | 212 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycolac® MG94 ABS Superior flow, injection molding ABS. Good impact. For thin-wall applications. |
|||
Vicat Softening Point | 100 °C @Load 5.10 kg |
212 °F @Load 11.2 lb |
50°C/h; ISO 306/B50 |
Radici Raditer® B RVA 100 Polybutylene Terephthalate with 10% Glass fiber Raditer® B RVA is a range of glass fiber reinforced Polybutylene terephthalate blends for injection molding, with excellent dimensional stability, low warpage and good surface aspect.Information pr.. |
|||
Vicat Softening Point | 100 °C @Load 1.00 kg |
212 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Flexirene® FG 20 I Butene Copolymer Linear Low Density Polyethylene Flexirene FG 20 I is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 I is recommended for the .. |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM D1525 |
Huntsman PE1065 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with excellent optical and machinability.Applications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms to FDA regu.. |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM D1525 |
Kolon DIAMAT® IM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM D1525 |
Ineos Nova 5410 High Impact Polystyrene High impact, Good ESCR, Good printabilityApplications: Thermoformed containers and lids, Hot and cold beverages cups, Custom sheetProperties were determined on injection molded specimens at 23°C .. |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM D1525 |
Lucky CF-920 Acrylic May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability. |
|||
Vicat Softening Point | 100 °C @Load 5.00 kg |
212 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical 80HF SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
Vicat Softening Point | 100 °C @Load 5.00 kg |
212 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance Feature: Injection Molding, Flame Retardant, Heat ResistanceApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 9001-96-2, 68928-70-1, and 1309-64-4Inf.. |
|||
Vicat Softening Point | 100 °C @Temperature 50.0 °C |
212 °F @Temperature 122 °F |
ISO 306 |
Styrolution Terluran® HD-15 ABS Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Vicat Softening Point | 100 °C | 212 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® ST-0185 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 100 °C | 212 °F | ISO 306 |
SIDPEC EGYPTENE® LL 0205 AF LLDPE Film Applications:Heavy duty sacks, mulch filmsStretch film, liners, geomembraneFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l... |
|||
Vicat Softening Point | 100 °C | 212 °F | B/120; ISO R306 |
Samsung Cheil Industries Starex® BF-0679P MABS, Unreinforced Scratch Resistant Scratch resistant material that is used for the exterior material of flat TVInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 100 °C | 212 °F | 1kg / 120°C; ASTM D1525 |
Supreme Petrochem SH 825 High Impact Polystyrene Characteristics Good flow properties Very good stiffness High heat grade Processing MoldingApplications Home appliances, lamp shades, wall clocks Gift sets, picnic boxes Air cooler, watch casesM.. |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM D1525 |
PlastxWorld CEVIAN® SER91 ABS General purpose and flame retarded ABS with excellent moldability and no plate-out.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Informat.. |
|||
Vicat Softening Point | 100 °C | 212 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D1525 |
Eastman Tenite Acetate 105E2R30025 Natural, Trsp Cellulose Acetate Plasticizer 33%. Weight loss on heating = 3.6% per ASTM D 707. Soluble matter loss = 0.6% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Vicat Softening Point | 100 °C | 212 °F | Rate A (50°C/h), Loading 1 (10 N); ASTM D1525 |
Entec Hyrene® PS-HI 8/2 High Impact Polystyrene Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM D1525 |
Dow TUFLIN™ HS-7021 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7021 NT 7 is an ethylene-hexene-1 copolymer designed.. |
|||
Vicat Softening Point | 100 °C | 212 °F | |
BASF Procom® C40H 451 Polypropylene Used for: instrument panels, motor vehicle grills, heater boxes.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM D1525 |
Americas Styrenics STYRON A-TECH® 1400AS High Impact Polystyrene Product CharacteristicsHigh FlowGood ImpactFood Contact CompliantTypical ApplicationsTelevision housingsPrinter HousingsConsumer goodsInformation provided by AmericasStyrenics LLC. |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM D1525 |
C.O.I.M. LARIPUR® LPR9060EF PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM D-1525 |
Plaskolite West Optix® CA - 2000 HF-4-2 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM D1525 |
Ineos Nova 5470 High Impact Polystyrene
(discontinued **) High impact, Good ESCR, Good printabilityApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheetProperties were determined on injection molded specimens at 23°C and.. |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM D648 |
Ineos Nova 8049 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High gloss at 60°=95; at 20°C=90, Improved scuff resistance, Custom colorsApplications: Injection molding, Cost effective replacement for some ABS applications, Excellent for applications where hi.. |
|||
Vicat Softening Point | 100 °C @Thickness 2.00 mm |
212 °F @Thickness 0.0787 in |
molded plaque, cured 20 hr at 100°C.; ASTM D1525 |
BASF Elastollan® 1185A10U Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Vicat Softening Point | 100 °C | 212 °F | |
BASF Procom® D 1026 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 100 °C | 212 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® NH-3208GL PC, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM D1525 |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 33% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |
|||
Vicat Softening Point | 100 °C | 212 °F | ASTM D1525 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |