Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 245 °C | 473 °F | STN EN ISO 306 |
Plastcom SLOVAMID® 6 NG1 GF 30 HLS PA6 reinforced with glass fiber, UV stabilized, hydrolysis resistant PA 6 for injection molding, reinforced with 30% glass fiber, for moldings used in the automotive, weather and UV stabilized. Determined for using in outside automotive applications like door handle,.. |
|||
Vicat Softening Point | 245 °C | 473 °F | 49 N; ISO 306, ASTM D1525 |
Nilit Nilamon A3 H K8 40% Mineral Reinforced PA66 Description: Nilamon A3 H K8 combines good stiffness with low warpage. It is used for applications which need a degree of rigidity, particularly at higher temperatures, but which need to stay flat a.. |
|||
Vicat Softening Point | 245 °C | 473 °F | 9.8 N; ASTM D1525 |
Nilit Polynil® C50 PA66/6 Co-Polymer Description: NYLON 66/6 copolymerApplication: CompoundingInformation provided by NILIT. |
|||
Vicat Softening Point | 245 °C @Load 5.10 kg |
473 °F @Load 11.2 lb |
50°C/h |
Radici Radilon® A RV250 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Vicat Softening Point | 245 °C @Load 5.10 kg |
473 °F @Load 11.2 lb |
50°C/h |
Radici Radilon® A RV300R (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Vicat Softening Point | 245 °C | 473 °F | ISO 306/A50 |
PolyOne Bergamid™ A700 G20 HW UF Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Vicat Softening Point | 245 °C | 473 °F | ISO 306/B50 |
PolyOne Bergamid™ A700 G20 HW UF Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Vicat Softening Point | 245 °C @Load 5.00 kg |
473 °F @Load 11.0 lb |
|
LATI Latamid 66 H2 G/50-V0HF1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Eu.. |
|||
Vicat Softening Point | 245 °C @Load 5.00 kg |
473 °F @Load 11.0 lb |
|
LATI Latamid 66 H2 G/25-V0HF1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good mechanical properties. Very good electrica.. |
|||
Vicat Softening Point | 245 °C @Load 5.00 kg |
473 °F @Load 11.0 lb |
|
LATI Latigloss 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Vicat Softening Point | 245 °C @Load 5.00 kg |
473 °F @Load 11.0 lb |
|
LATI Latilub 66 Y/20 PA66, Aramid Fiber Reinforced Self-lubricating product based on Polyamide 66 (PA66). Aramid fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termo.. |
|||
Vicat Softening Point | 245 °C @Load 5.00 kg |
473 °F @Load 11.0 lb |
|
LATI Latilub 66-10T Y/15 PA66, 15% Aramid Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). PTFE. Aramid fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri.. |
|||
Vicat Softening Point | 245 °C @Load 5.00 kg |
473 °F @Load 11.0 lb |
|
LATI Latilub 66-20T PA66, PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastic.. |
|||
Vicat Softening Point | 245 °C @Load 5.00 kg |
473 °F @Load 11.0 lb |
|
LATI Latilub 80-10T Y/15 PPS, 15% Aramid Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Vicat Softening Point | 245 °C @Load 5.00 kg |
473 °F @Load 11.0 lb |
|
LATI Latishield 66-10A G/15 PA66, Steel/Glass Fiber Reinforced EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Vicat Softening Point | 245 °C @Load 5.00 kg |
473 °F @Load 11.0 lb |
|
LATI Latishield 66-10A H2 CETG/400 PA66, Steel/Glass Fiber Reinforced, Mineral Filled, Heat Stabilized EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri.. |
|||
Vicat Softening Point | 245 °C | 473 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL GTX GTX909 PPE+PS+PA (Asia Pacific) 400F (205C) HDT. 3.3 Notched Izod. Excellent chemical resistance |
|||
Vicat Softening Point | 245 °C | 473 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Vicat Softening Point | 245 °C | 473 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Asia Pacific) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Vicat Softening Point | 245 °C | 473 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Noryl GTX GTX918WR PPE+PS+PA (Asia Pacific) High flow PPE+PS+PA for under-the-hood and electrical applications. With mold releaseThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 245 °C | 473 °F | ISO 306 |
Tisan TISLAMID® 66 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Vicat Softening Point | 245 °C | 473 °F | ISO 306 |
Tisan TISLAMID® 66 30% Glass Bead Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Vicat Softening Point | 245 °C | 473 °F | DAM; 50°C/h 50N; ISO 306 |
DuPont Performance Polymers Zytel® FG50 NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Vicat Softening Point | 245 °C | 473 °F | B/120; ISO 306 |
Eurostar Staramide AG3X3 PA66, Glass Fiber Reinforced, Impact Modified, Injection Molding Staramide AG3X3 is an Impact Modified, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Vicat Softening Point | 245 °C @Load 5.10 kg |
473 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NA40 MF40 BK001 HS PA6.6, 40% mineral filled, heat stabilized, black Information provided by Eurotec® |
|||
Vicat Softening Point | 245 °C @Load 5.10 kg |
473 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NA40 NL FA50 PA6.6, unfilled, flame retardant - halogen free, natural Information provided by Eurotec® |
|||
Vicat Softening Point | 245 °C @Load 5.10 kg |
473 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NA40 NL XA70 PA6.6, unfilled, flame retardant - halogen free (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Vicat Softening Point | 245 °C | 473 °F | 50N; ISO 306 |
Eurotec® Tecomid® NA40 NL XA 20 PA 6.6 unreinforced, UL94 V0 Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Vicat Softening Point | 245 °C @Load 5.10 kg |
473 °F @Load 11.2 lb |
ISO 306 |
Eurotec® Tecomid® NT40 NL PPA, unfilled, natural Information provided by Eurotec® |
|||
Vicat Softening Point | 245 °C @Load 5.10 kg |
473 °F @Load 11.2 lb |
50°C/h |
Radici Radilon® A RV400 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |