Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | >= 220 °C @Load 5.001 kg |
>= 428 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANAMID 66 A12^ F15 Nylon 66, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 220 °C | 428 °F | 9.8 N; ISO 306, ASTM D1525 |
Nilit Nilamid B3 H G3 15% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 6. These products combine good overall mechanical performance and impact strength with ease of processing. Key cha.. |
|||
Vicat Softening Point | 220 °C | 428 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 3-7088-1 Polyamide 6, with carbon fiber and glass fiber, low-warpage Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall.. |
|||
Vicat Softening Point | 220 °C @Load 5.00 kg |
428 °F @Load 11.0 lb |
|
LATI Lapex R G/20 PPSU, 20% Glass Reinforced Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Vicat Softening Point | 220 °C | 428 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1100-8049 Polyether sulfone, with glass fiber Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 2200F PEI 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics ULTEM CRS5011R PEI Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics ULTEM CRS5201R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS com.. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics ULTEM CRS5311 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS compliant. UL94 V0 and 5VA li.. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics ULTEM HU2110 PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics ULTEM HU2310 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Valox® 325 PBT (Europe-Africa-Middle East) VALOX 325 is a general purpose, unreinforced PBT injection moulding resin. Applications: sprinklers and nozzles, pumps, doorhandles, tank covers, pens and pencils. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate A/50; ASTM D1525 |
SABIC Innovative Plastics Valox® 325 PBT (Europe-Africa-Middle East) VALOX 325 is a general purpose, unreinforced PBT injection moulding resin. Applications: sprinklers and nozzles, pumps, doorhandles, tank covers, pens and pencils. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate A/50; ASTM D1525 |
SABIC Innovative Plastics Valox® 325FC PBT (Europe-Africa-Middle East) Commercial, VALOX 325FC is compliant with food contact regulations. VALOX 325FC is a general purpose, unreinforced PBT injection moulding resin which contains internal mold release. This new 325FC g.. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Valox® SHF4340 PBT (Europe-Africa-Middle East) 20% GF Super High Flow PBT |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate A/50; ASTM D1525 |
SABIC Innovative Plastics Valox® SHF4340 PBT (Europe-Africa-Middle East) 20% GF Super High Flow PBT |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX820 PPE+PA (Europe-Africa-Middle East) NORYL GTX820 is a 20% glass reinforced grade with excellent chemical resistance in combination with high stiffness and heat resistance. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PA (Europe-Africa-Middle East) NORYL GTX830 a 30% glass reinforced grade which offers an excellent combination of chemical/heat resistance in combination with stiffness. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Asia Pacific) Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A.. |
|||
Vicat Softening Point | 220 °C | 428 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Europe-Africa-Middle East) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Vicat Softening Point | 220 °C @Load 5.00 kg |
428 °F @Load 11.0 lb |
|
LATI Lapex A G/30 PES, 30% Glass Fiber Reinforced Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |
|||
Vicat Softening Point | 220 °C @Load 5.10 kg |
428 °F @Load 11.2 lb |
50°C/h |
Radici Radiflam® A AE (dry) Nylon 66 Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g.. |