Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 218 °C | 424 °F | B; STN EN ISO 306 |
Plastcom SLOVAMID 6 LI/1 Polyamide 6, Impacted FeaturesPA 6 with the content of thermoplastic elastomer. Impacted, for mouldings with high toughness either at low temperatures, suitable for external use, eg. ski shoes, sports and safety helmets.. |
|||
Vicat Softening Point | 218 °C | 424 °F | 50°C/h 50N |
Covestro Apec® DP 1-9389 Polycarbonate
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and ha.. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 1000F PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer.. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Ultem 1000FV PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Ultem 1000FV PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 1000P PEI Standard flow Polyetherimide (Tg 217C) in 350 micron powder. ECO Conforming. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 1000P PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) in 350 micron powder. ECO Conforming. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 1000R PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 1000R PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 1000RV PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 1000RV PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 1010 PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer be .. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 1010R PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Ultem 1010RV PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics ULTEM 2200F PEI 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics ULTEM 2200F PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with b.. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics ULTEM 2210 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics ULTEM 2210F PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with b.. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics ULTEM 2210K PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM HU1000 PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics ULTEM HU2200 PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Asia Pacific) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Europe-Africa-Middle East) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Vicat Softening Point | 218 °C | 424 °F | ASTM D1525 |
Tipco Tipcofil® AG 800 - 40% Glass Fiber Reinforced Nylon-6 Compound, with High Heat Stability 40% Glass Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Vicat Softening Point | 218 °C | 424 °F | ISO 306/A50 |
Premix Thermoplastics PRE-ELEC® PA 1411 Conductive Thermoplastic Compound PRE-ELEC® PA 1411 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. PRE-ELEC® PA 1411 has a very low electrical resistivity. P.. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 1000E PEI Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact compliant, NSF 51 Listing. Effective June, 2007 this grade will no longer.. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 1000 PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing, compliant in natural color. Effective June, 20.. |
|||
Vicat Softening Point | 218 °C | 424 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics ULTEM 1010M PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. |