Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 190 °C | 374 °F | B |
Plastcom SLOVASTER® E GF 30 PBT, 30% glass fibre FeaturesPET for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Vicat Softening Point | 190 °C | 374 °F | ISO 306 |
Radici Radilon® SHS (dry) Nylon 6 General PurposeInformation provided by Radici group. |
|||
Vicat Softening Point | 190 °C | 374 °F | B; STN EN ISO 306 |
Plastcom SLOVAMID 6 BT LS Polyamide 6, UV Stabilized FeaturesPA 6 for injection moulding with the content of UV stabilizer predetermines products for external use, eg. seats for sport stadiums, covers of electrical appliances. Delivered in natural an.. |
|||
Vicat Softening Point | 190 °C @Load 5.00 kg |
374 °F @Load 11.0 lb |
|
LATI Latistat 67-08 PA66, Impact Modified Dissipative product based on Polyamide 66 (PA66), impact modified. Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr.. |
|||
Vicat Softening Point | 190 °C | 374 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 190 °C | 374 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® 815F PBT+PET PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Vicat Softening Point | 190 °C | 374 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Asia Pacific) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Vicat Softening Point | 190 °C | 374 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Europe-Africa-Middle East) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Vicat Softening Point | 190 °C | 374 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA (Asia Pacific) NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance. |
|||
Vicat Softening Point | 190 °C | 374 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX918WR PPE+PA (Asia Pacific) High flow PPE+PA for under-the-hood and electrical applications. With mold release |
|||
Vicat Softening Point | 190 °C | 374 °F | |
Tipco Tipcofil® AU 027 - Unfilled Nylon-6 Compound, with High Heat Stability, for Injection Molding Unreinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Vicat Softening Point | 190 °C | 374 °F | ASTM D1525 |
Toyobo PELPRENE™ P150B Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Vicat Softening Point | 190 °C | 374 °F | 50°C/h 10N; ISO 306 |
DSM Arnitel® EM550 55 Shore D, Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Vicat Softening Point | 190 °C | 374 °F | 50°C/h 10N; ISO 306 |
DSM Arnitel® EM550 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Vicat Softening Point | 190 °C | 374 °F | 50°C/h 50N |
Covestro Texin® 260 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop.. |
|||
Vicat Softening Point | 190 °C | 374 °F | B/120; ISO 306 |
Eurostar Staramide AST44 PA66, Impact Modified, Injection Molded AST44 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Vicat Softening Point | 190 °C | 374 °F | 50N; ISO 306 |
Eurotec® Tecodur® PB70 GR15 NL TD 28 PBT 15% glass fiber reinforced, UL94 V0, impact modified, high CTI Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Vicat Softening Point | 190 °C @Load 5.10 kg |
374 °F @Load 11.2 lb |
ISO 306 |
Azoty Tarnow™ Tarnamid® T-29 MCS Polyamide 6 - Colored Colored medium-high viscosity grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration damping capac.. |
|||
Vicat Softening Point | 190 °C | 374 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA (Europe-Africa-Middle East) NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance. |