Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 170 °C @Load 5.10 kg |
338 °F @Load 11.2 lb |
50°C/h |
Radici Radilon® S ESL128 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Asia Pacific) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Asia Pacific) XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Europe-Africa-Middle East) XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Vicat Softening Point | 170 °C | 338 °F | 49 N; ISO 306, ASTM D1525 |
Nilit Nilamid B3 H XB Unfilled, Impact Resistant PA6 Description: Nilamid B3 H XB is a high impact NYLON 6. The product has excellent impact properties above 0°C, combined with good maintaining mechanical characteristics. Application areas include au.. |
|||
Vicat Softening Point | 170 °C | 338 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 50-8025 Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Vicat Softening Point | 170 °C | 338 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 6-7595 Polyamide 12, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic.. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Ultem ATX100F PEI (Europe-Africa-Middle East) Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. US FDA Food Contact Compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Ultem HATX100 PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® HX3091HP PBT PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity at 250C and 21.6kgf is 3500-4500 poise. Available in Natural color (1001) only. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate A/50; ASTM D1525 |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® VIC4311 PBT VALOX VIC4311 is a 30% glass filled, impact modified PBT with excellent epoxy adhesion. Automotive underhood applications such as ignition coil housings. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL PX300 PPE+HIPS (Asia Pacific) Low odor grade for IC tray application |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® V3004 PBT (Asia Pacific) Unfilled PBT modified with elastomer. Targeted for flexible hinge, automotive connectors, film applications. |
|||
Vicat Softening Point | 170 °C | 338 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Vicat Softening Point | 170 °C | 338 °F | ASTM D1525 |
Toyobo PELPRENE™ P50DFR Polyester TPE, Flame Resistant Features: Polyester TPE, Flame ResistantInformation provided by Toyobo. |
|||
Vicat Softening Point | 170 °C @Load 1.00 kg |
338 °F @Load 2.20 lb |
ASTM D1525 |
Eastman Eastman AP006 Copolyester Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly.. |
|||
Vicat Softening Point | 170 °C | 338 °F | 1kg load; ASTM D1525 |
Eastman Neostar FN005 Elastomer Neostar FN005 elastomer is a tough, clear, durable copolyester ether. It was designed for use in the profile and automotive markets, but is also used in packaging and tubing applications where tough.. |
|||
Vicat Softening Point | 170 °C | 338 °F | 50 N; ISO 306 |
CP-Polymer-Technik Wellamid® 6000/42 CP Nylon 6, Polymer Modified, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Vicat Softening Point | 170 °C | 338 °F | 50 N; ISO 306 |
CP-Polymer-Technik Wellamid® 6000/42 Nylon 6, Polymer Modified, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |