Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 160 °C | 320 °F | B |
Plastcom SLOVALEN PH 63 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |
|||
Vicat Softening Point | 160 °C | 320 °F | B |
Plastcom SLOVALEN PH 71 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shr.. |
|||
Vicat Softening Point | 160 °C | 320 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® 4501 PC (Europe-Africa-Middle East) LEXAN 4501 is a copolymer of polyphthalate carbonate resin for applications requiring high heat resistance. |
|||
Vicat Softening Point | 160 °C | 320 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® FXM2143H PC Copolymer FXM2143H is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C. |
|||
Vicat Softening Point | 160 °C | 320 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® HP9NR PC Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. For blow molding .. |
|||
Vicat Softening Point | 160 °C | 320 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Vicat Softening Point | 160 °C | 320 °F | B |
Plastcom SLOVALEN PH 91 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Vicat Softening Point | 160 °C | 320 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 50/CF/10/GF/20/BK Polycarbonate, with carbon fiber and glass fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Vicat Softening Point | 160 °C | 320 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 50/TF/15/NAT Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Vicat Softening Point | 160 °C | 320 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 50-3019 Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te.. |
|||
Vicat Softening Point | 160 °C | 320 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 50-7317 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Vicat Softening Point | 160 °C | 320 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 50-8300 Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te.. |
|||
Vicat Softening Point | 160 °C | 320 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 80-7655/RD Polyacetal-copolymer, with aramid reinforcement and PTFE, toughness-modified, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Vicat Softening Point | 160 °C | 320 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 80-7727 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Vicat Softening Point | 160 °C | 320 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 80-8444 Polyacetal-copolymer, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.dynamic stressReduced moment of inertia compared with metal parts.Isotropic shrinkage character.. |
|||
Vicat Softening Point | 160 °C | 320 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
Vicat Softening Point | 160 °C | 320 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL NH7010 PPE+PS (Asia Pacific) High heat, Non halogenated flame retardant Noryl product |
|||
Vicat Softening Point | 160 °C | 320 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL ENV150 PPE (Europe-Africa-Middle East) Noryl* ENV150 modified polyphenylene ether resin is an unfilled, flame retardant high heat grade suitable for extrusion molding conversion route. It uses non-chlorinated, non-brominated FR additives.. |
|||
Vicat Softening Point | 160 °C | 320 °F | 50°C/h 50N; ISO 306 |
DSM Arnitel® EM740 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Vicat Softening Point | 160 °C | 320 °F | 50°C/h 50N; ISO 306 |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo.. |
|||
Vicat Softening Point | 160 °C | 320 °F | 50°C/hr; 50N |
Arkema Group Rilsan® BMV Nylon 11 (Conditioned) Designation ISO 1874-PA11,M,18-010Rigid grade for injection molding. Available color: natural. Free additive.High impact strength. Easy filling of the mold due to its well adapted melt viscosity. Lo.. |
|||
Vicat Softening Point | 160 °C | 320 °F | 50°C/hr; 50N |
Arkema Group Rilsan® Powder D40 Natural Nylon 11, Coating Grade Powder D40 NATURAL - RILSAN POLYAMIDE 11 (PA11) POWDERUnpigmented and clear Powder as an additive for paints. Improves the scratch and abrasion resistance of paints. Allows for different texture d.. |
|||
Vicat Softening Point | 160 °C | 320 °F | ISO 306 |
BASF Ultraform® N2200 G43 POM Description: Is a POM, injection-molding grade for parts requiring high stiffness and strength together with good mold release.Information provided by BASF |
|||
Vicat Softening Point | 160 °C | 320 °F | ISO 306/A50 |
Addiplast Addilene H 511 V30 Polypropylene Homopolymer Glass fiber reinforced, high modulus and improved stiffnessInformation provided by Addiplast. |
|||
Vicat Softening Point | 160 °C | 320 °F | |
BASF Luranyl® KR 2460/3 Polyphenylene Ether + Styrene-Butadiene Blend Flame retardant grade with very high heat resistance; used for precision parts and where the material must withstand high injection temperatures (e.g. heater-fan impellers).Data was collected by ISO.. |
|||
Vicat Softening Point | 160 °C | 320 °F | B; STN EN ISO 306 |
Plastcom SLOVALEN PH 51 T 20 Polypropylene Homopolymer, 20% Mineral Filled FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filler. Increased rigidity, strength and thermal use up to 130°C. Decreased shrinkage. General application .. |
|||
Vicat Softening Point | 160 °C | 320 °F | B |
Plastcom SLOVALEN PH 73 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |
|||
Vicat Softening Point | 160 °C | 320 °F | DIN ISO 306 |
Lehmann & Voss PLASLUBE J-50/10/TF/15/BK Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te.. |