Mechanical Properties Metric English Comments
Shear Modulus 1.00 GPa

@Temperature 70.0 °C
145 ksi

@Temperature 158 °F
Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK605 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 NC010 is a 30% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P..
Shear Modulus 1.00 GPa

@Temperature 20.0 °C
145 ksi

@Temperature 68.0 °F
DAM; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66  (Unverified Data**)
14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica..
Shear Modulus 1.00 GPa

@Temperature 200 °C
145 ksi

@Temperature 392 °F
Akro-Plastic Akromid® T6 GF 50 (3106) PPA Dry, 50% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Shear Modulus 1.00 GPa

@Temperature 50.0 °C
145 ksi

@Temperature 122 °F
ISO 6721
BASF Ultrason E 6020 P PES
Ultrason E 6020 P is an unfilled, injection molding PES grade. Polyethersulfone flakes of high molecular weight and good solubility in typical solvents (N-Methylpyrrolidone, Dimethylacetamide, Dichl..
Shear Modulus 1.00 GPa

@Temperature 50.0 °C
145 ksi

@Temperature 122 °F
ISO 6721
BASF Ultrason® E 2010 C6 30% Carbon Filled
Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu..
Shear Modulus 1.00 GPa

@Temperature 50.0 °C
145 ksi

@Temperature 122 °F
ISO 6721
BASF Ultrason E 1010 PES
Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability.
Shear Modulus 1.00 GPa

@Temperature 50.0 °C
145 ksi

@Temperature 122 °F
ISO 6721
BASF Ultrason E 2010 G4 20% Glass Filled PES
Ultrason E 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength.
Shear Modulus 1.00 GPa

@Temperature 50.0 °C
145 ksi

@Temperature 122 °F
ISO 6721
BASF Ultrason E 2010 G6 30% Glass Filled PES
Ultrason E 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength.
Shear Modulus 1.00 GPa

@Temperature 50.0 °C
145 ksi

@Temperature 122 °F
ISO 6721
BASF Ultrason E 2010 PES
Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req..
Shear Modulus 1.00 GPa

@Temperature 50.0 °C
145 ksi

@Temperature 122 °F
ISO 6721
BASF Ultrason E 3010 PES
Ultrason E 3010 is an unfilled, higher viscosity injection molding and extrusion PES grade, tougher and with improved chemical resistance.
Shear Modulus 1.00 GPa

@Temperature 50.0 °C
145 ksi

@Temperature 122 °F
ISO 6721
BASF Ultrason E 2020 P PES
Ultrason E 2020 P is an unfilled, injection molding PES grade. Polyethersulfone flakes, for solvent based processes; product is soluble e.g. in N-Methylpyrrolidone and N,N-Dimethylacetamide.